MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Braskem RPL 5A1 NL Recycled Low Density Polyethylene
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Blow Molding Grade

Material Notes: RPR 5A1 NL is Low Density Polyethylene resin containing 50% Post-Consumer Recycled (PCR) LDPE. Its properties are comparable to virgin LDPE resins.
Applications: Shrink film.
Processes: Blow film extrusion.

Film properties tested with a monolayer 50 µm thickness blown film, blow up ratio: 2.8, die gap: 1.8 mm.

Information provided by Braskem.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.921 g/cc0.0333 lb/in³ASTM D792
Melt Flow 0.60 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.60 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 200 %200 %ASTM D882
Film Elongation at Break, TD 591 %591 %ASTM D882
Elmendorf Tear Strength TD 550 g550 gASTM D1922
Dart Drop Test 93.0 g0.205 lbASTM D1709/A
Film Tensile Strength at Break, MD 15.0 MPa2180 psiASTM D882
Film Tensile Strength at Break, TD 17.0 MPa2470 psiASTM D882
1% Secant Modulus, MD 151 MPa21900 psiASTM D882
1% Secant Modulus, TD 591 MPa85700 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 22 %22 %ASTM D1003
 
Descriptive Properties
Film Contraction (%)18TD
 82MD

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBRAS608 / 314001

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.