MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow SURLYN™ 1605SBR-E Ionomer
Categories: Polymer; Thermoplastic; Ionomer; Ionomer, Film Grade

Material Notes: Product Description: SURLYN™ 1605SBR-E is an ionomer of ethylene acid copolymer. The resin can be processed in conventional blown film, cast film, sheet extrusion and coextrusion equipment designed to process polyethylene and ethylene copolymer type resins. It is also used in extrusion coating and coextrusion coating equipment designed to process polyethylene and ethylene copolymer type resins.
Features: Sodium Ionomer
Characteristics/Benefits: Contains slip, antiblock, and chill roll release additives

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Additive: Antiblock; Chill Roll Release; Slip

Agency Ratings: FDA 21 CFR 177.1330(a)

Form: Pellets

Processing Method: Blown Film; Cast Film; Coextrusion; Extrusion Coating; Sheet Extrusion

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³ISO 1183
 0.952 g/cc0.0344 lb/in³ASTM D792
Melt Flow  3.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 3.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Thermal PropertiesMetricEnglishComments
Melting Point 61.1 °C142 °FFreezing point; ASTM D3418
 61.1 °C142 °FFreezing point; ISO 3146
 93.9 °C201 °FPeak; ASTM D3418
 93.9 °C201 °FISO 3146
Vicat Softening Point 63.9 °C147 °FASTM D1525
 63.9 °C147 °FISO 306
 
Descriptive Properties
Ion TypeSodium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOWF562 / 311255

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.