MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

ZEON Hydrin® H65 Epichlorohydrin Elastomer (ECO)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Hydrin H65 is an epichlorohydrin homopolymer with high oil, fuel and solvent resistance. Compounds using Hydrin H65 typically exhibit good heat resistance, excellent ozone resistance along with outstanding gas permeability. Hydrin H65 is supplied as bales sealed in an LDPE bag free.

Hydrin® epichlorohydrin (ECO) elastomers provide an excellent balance of heat (125°C), oil, fuel, and ozone resistance with superior low temperature flexibility. Hydrin is broadly used in automotive fuel hose, air ducts, A/C, and vibration dampening. Its electrical properties benefit laser printer rolls. Hydrin is classified as a CH polymer according to SAE J200 / ASTM D2000.

Information provided by Zeon Chemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Mooney Viscosity 60 - 70
@Temperature 100 °C
60 - 70
@Temperature 212 °F
ML(1+4); MBL 1414/ASTM D-1646
Ash <= 0.50 %<= 0.50 %MBL 1358
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 125 °C257 °F
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 1.0 %<= 1.0 %MBL 1361

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PZEON939 / 250118

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.