MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Aluminum 1050-H18
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 1000 Series Aluminum

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
The aluminum content for unalloyed aluminum not made by a refining process is the difference between 100.00 percent and the sum of all other analyzed metallic elements present in amounts of 0.010 percent of more each, expressed to the second decimal before determining the sum. For alloys and unalloyed aluminum not made by a refining process, when the specified maximum limit is 0.XX, an observed value or a calculated value greater than 0.005 but less than 0.010% is rounded off and shown as " less than 0.01%".
Composition information provided by the Aluminum Association and is not for design.

Key Words: Aluminum 1050-H18; Aluminium 1050-H18; UNS A91050; NF A5 (France); DIN Al99.5; AA1050-H18, ASTM B491; BS 1B (UK); CSA 9950 (Canada); Al1050-H18
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.705 g/cc0.09772 lb/in³AA; Typical
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 4343500 kg load with 10 mm ball. Calculated value.
Tensile Strength, Ultimate 160 MPa23200 psi
Tensile Strength, Yield 145 MPa21000 psi
Elongation at Break 7.0 %
@Thickness 1.60 mm
7.0 %
@Thickness 0.0630 in
In 5 cm
Tensile Modulus 69.0 GPa10000 ksiCompressive Modulus is about 2% higher
Poissons Ratio 0.330.33
Shear Modulus 26.0 GPa3770 ksiEstimated from similar Al alloys.
Shear Strength 83.0 MPa12000 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000290 ohm-cm0.00000290 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 390 J/g168 BTU/lb
CTE, linear  21.8 µm/m-°C
@Temperature -50.0 - 20.0 °C
12.1 µin/in-°F
@Temperature -58.0 - 68.0 °F
 23.6 µm/m-°C
@Temperature 20.0 - 100 °C
13.1 µin/in-°F
@Temperature 68.0 - 212 °F
 24.5 µm/m-°C
@Temperature 20.0 - 200 °C
13.6 µin/in-°F
@Temperature 68.0 - 392 °F
 25.5 µm/m-°C
@Temperature 20.0 - 300 °C
14.2 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.900 J/g-°C0.215 BTU/lb-°F
Thermal Conductivity 227 W/m-K1580 BTU-in/hr-ft²-°F
Melting Point 646 - 657 °C1190 - 1210 °F
Solidus 646 °C1190 °F
Liquidus 657 °C1210 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al >= 99.50 %>= 99.50 %Specified
Copper, Cu <= 0.05 %<= 0.05 %
Iron, Fe <= 0.40 %<= 0.40 %
Magnesium, Mg <= 0.05 %<= 0.05 %
Manganese, Mn <= 0.05 %<= 0.05 %
Other, each <= 0.03 %<= 0.03 %
Silicon, Si <= 0.25 %<= 0.25 %
Titanium, Ti <= 0.03 %<= 0.03 %
Vanadium, V <= 0.05 %<= 0.05 %
Zinc, Zn <= 0.05 %<= 0.05 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 1050-O
Aluminum 1050-H14
Aluminum 1050-H16
Aluminum 6061-T6; 6061-T651
Titanium Ti-6Al-4V (Grade 5), Annealed

MA1050H18 / 8722

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.