MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Phillips Sumika Marlex® CBF-300 Talc-Filled High Flow Thermoplastic Olefin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Applications:
  • Automotive exterior fascias

Information provided by Chevron Phillips.

Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. This product had been discontinued prior to the shutdown announcement.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc
@Thickness 3.17 mm
0.0368 lb/in³
@Thickness 0.125 in
injection molded specimen; ISO 1183
Melt Flow 30 g/10 min
@Load 2.16 kg,
Temperature 230 °C
30 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 606015 second dwell; ISO 868
Tensile Strength, Yield 16.0 MPa
@Thickness 3.17 mm
2320 psi
@Thickness 0.125 in
50 mm/min, injection molded specimen; ISO 527
Flexural Modulus 1.25 GPa
@Thickness 3.17 mm
181 ksi
@Thickness 0.125 in
injection molded specimen, 2 mm/min; ISO 178
Izod Impact, Notched (ISO)  4.00 kJ/m²
@Thickness 3.17 mm,
Temperature -40.0 °C
1.90 ft-lb/in²
@Thickness 0.125 in,
Temperature -40.0 °F
ISO 180
 44.0 kJ/m²
@Thickness 3.17 mm,
Temperature 23.0 °C
20.9 ft-lb/in²
@Thickness 0.125 in,
Temperature 73.4 °F
ISO 180
Impact Test  17.0 J
@Temperature 23.0 °C
12.5 ft-lb
@Temperature 73.4 °F
Instrumented, 2.2 m/s, ductile; ASTM D3763
 24.0 J
@Temperature -30.0 °C
17.7 ft-lb
@Temperature -22.0 °F
Instrumented, 2.2 m/s, ductile; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 84.0 °C
@Thickness 3.17 mm
183 °F
@Thickness 0.125 in
injection molded specimen; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 51.0 °C
@Thickness 3.17 mm
124 °F
@Thickness 0.125 in
injection molded specimen; ISO 75

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow AFFINITY™ EG 8185 Polyolefin Plastomer (POP)
Dow AFFINITY™ EG 8200G Ethylene alpha-olefin copolymer
Dow AFFINITY™ GA 1900 Polyolefin Plastomer (POP)
Dow AFFINITY™ GA 1950 Polyolefin Plastomer (POP)
Dow AFFINITY™ PF 1140G Polyolefin Plastomer (POP)

PCHEVD072 / 20662

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.