MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Mocom (ALBIS) ALTECH® PA6 A 2015/310 GF15 IM Nylon 6, 15% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Glass Fiber Filled

Material Notes: Base Polymer: Polyamide 6

Filler/Additive System: 15% glass fibers

Special Features: Heat ageing stabilization, impact modified, injection molding grade

Market Segment: Machinery, Electrical and Electronic

Application Area: Injection molded parts, Power tools

Typical Application: Housings, operating elements, impact protection/shock absorber

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
@Time 86400 sec
0.0030 - 0.0050 in/in
@Time 24.0 hour
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 - 0.0090 cm/cm
@Time 86400 sec
0.0070 - 0.0090 in/in
@Time 24.0 hour
ISO 294-4
Storage Temperature <= 30.0 °C<= 86.0 °Fdry, protected from light
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 84.0 MPa12200 psiISO 527
Elongation at Break 4.5 %4.5 %ISO 527
Tensile Modulus 4.60 GPa667 ksiISO 527
Flexural Strength 130 MPa18900 psiISO 178
Flexural Modulus 3.80 GPa551 ksiISO 178
Charpy Impact Unnotched  6.50 J/cm²
@Temperature 23.0 °C
30.9 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
 8.00 J/cm²
@Temperature -40.0 °C
38.1 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1eU
Charpy Impact, Notched  0.850 J/cm²
@Temperature -40.0 °C
4.04 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1eA
 2.00 J/cm²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 221 °C430 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 190 °C374 °FISO 75-1/-2
Vicat Softening Point 200 °C392 °FB50; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 270 - 290 °C518 - 554 °FInjection molding
Mold Temperature 80.0 - 90.0 °C176 - 194 °FInjection molding
Drying Temperature  60.0 - 80.0 °C
@Time 7200 - 21600 sec
140 - 176 °F
@Time 2.00 - 6.00 hour
in a dry air (desiccant) dryer
 60.0 - 80.0 °C
@Time 7200 - 21600 sec
140 - 176 °F
@Time 2.00 - 6.00 hour
in an circulating dryer
 
Descriptive Properties
Base PolymerPolyamide 6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PALBIS8653 / 242712

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.