MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Tetrachlorosilane (Silicon tetrachloride), SiCl4
Categories: Fluid; Solvent

Material Notes: CAS Number: 10026-04-7

Physical Form: Colorless Fuming Liquid

Key Words: SiCl4
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.48 g/cc0.0535 lb/in³
Molecular Weight 169.897 g/mol169.897 g/mol
Vapor Pressure 0.257974 bar
@Temperature 20.0 °C
193.497 torr
@Temperature 68.0 °F
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 35.9800 bar26987.2 torr
Critical Temperature 235.1 °C455.2 °F
Critical Density 0.521 g/cc0.0188 lb/in³
Critical Molar Volume 326 cm³/mol19.9 in³/mol
 
Electrical PropertiesMetricEnglishComments
Magnetic Susceptibility -0.0000875-0.0000875cm^3/mol
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 44.73 J/g19.24 BTU/lb
Heat of Vaporization 168.9 J/g72.67 BTU/lbAt Boiling Point
 174.8 J/g
@Temperature 25.0 °C
75.20 BTU/lb
@Temperature 77.0 °F
Specific Heat Capacity 0.5315 J/g-°C0.1270 BTU/lb-°FGas
 0.8552 J/g-°C0.2044 BTU/lb-°FCrystal
Thermal Conductivity 0.101 W/m-K
@Temperature 20.0 °C
0.701 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point -68.85 °C-91.93 °F
Boiling Point 57.65 °C135.8 °F
Heat of Formation -687 kJ/mol-687 kJ/molCrystal
 -657 kJ/mol-657 kJ/molGas
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter15.8019
Antoine's Vapor Pressure B Parameter2634.16
Antoine's Vapor Pressure C Parameter-43.15
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
Critical Compressibility (Zc)0.29
Molar Heat Capacity (298K)0 J/mol-K
SolubilityReacts with H2O

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Gold, Au
Gallium, Ga

EINOR3080 / 5177

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.