MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

303 MA Stainless Steel, in bar, annealed
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T 300 Series Stainless Steel

Key Words: T303, T 303, 303SS, 303 SS, UNS S30345, ASTM A581 (XM-2), ASTM A582 (XM-2), 18-8, 18/8
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.81 g/cc0.282 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 160160
Hardness, Knoop 180180Converted from Brinell
Hardness, Rockwell B 8383Converted from Brinell
Hardness, Vickers 167167Converted from Brinell
Tensile Strength, Ultimate 620 MPa89900 psi
Tensile Strength, Yield 275 MPa
@Strain 0.2 %
39900 psi
@Strain 0.2 %
Elongation at Break 50 %50 %in 50 mm
Modulus of Elasticity 190 GPa27600 ksi
Izod Impact  115 J
@Temperature 21.0 °C
84.8 ft-lb
@Temperature 69.8 °F
 150 J
@Temperature -195 °C
111 ft-lb
@Temperature -319 °F
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000805 ohm-cm0.0000805 ohm-cmannealed, 0.000083 cold drawn
Magnetic Permeability 1.0081.008at RT
 
Thermal PropertiesMetricEnglishComments
CTE, linear  16.4 µm/m-°C
@Temperature 21.0 - 315 °C
9.11 µin/in-°F
@Temperature 69.8 - 599 °F
 17.2 µm/m-°C
@Temperature 20.0 °C
9.56 µin/in-°F
@Temperature 68.0 °F
 18.5 µm/m-°C
@Temperature 21.0 - 540 °C
10.3 µin/in-°F
@Temperature 69.8 - 1000 °F
 19.1 µm/m-°C
@Temperature 21.0 - 650 °C
10.6 µin/in-°F
@Temperature 69.8 - 1200 °F
Specific Heat Capacity 0.500 J/g-°C
@Temperature 0.000 - 100 °C
0.120 BTU/lb-°F
@Temperature 32.0 - 212 °F
Thermal Conductivity  16.2 W/m-K
@Temperature 100 °C
112 BTU-in/hr-ft²-°F
@Temperature 212 °F
 21.5 W/m-K
@Temperature 500 °C
149 BTU-in/hr-ft²-°F
@Temperature 932 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.80 %0.80 %
Carbon, C 0.15 %0.15 %
Chromium, Cr 18 %18 %
Iron, Fe 68 %68 %
Manganese, Mn 2.0 %2.0 %
Molybdenum, Mo 0.50 %0.50 %
Nickel, Ni 9.0 %9.0 %
Phosphorus, P 0.040 %0.040 %
Silicon, Si 1.0 %1.0 %
Sulfur, S 0.14 %0.14 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
303 Stainless Steel, annealed bar
Copper, Cu; Annealed
303 Stainless Steel, annealed
316 Stainless Steel, annealed bar
303 Stainless Steel, cold drawn bar

MQ303Q / 12672

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.