MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Cast Stainless Steel A872, ASTM A872
Categories: Metal; Ferrous Metal; Stainless Steel; Cast Stainless Steel

Material Notes: Centrifugally Cast Ferritic-Austenitic Pipe, Corrosion Resistant; KCR-D183

Key Words: ASTM A872 (97)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell <= 297<= 297
Tensile Strength, Ultimate >= 620 MPa>= 89900 psi
Tensile Strength, Yield >= 450 MPa>= 65300 psi
Elongation at Break >= 20 %>= 20 %
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.030 %<= 0.030 %
Chromium, Cr 23 - 26 %23 - 26 %
Cobalt, Co 0.50 - 1.5 %0.50 - 1.5 %
Copper, Cu <= 1.0 %<= 1.0 %
Iron, Fe 55.2 - 69.4 %55.2 - 69.4 %As remainder
Manganese, Mn <= 2.0 %<= 2.0 %
Molybdenum, Mo 2.0 - 4.0 %2.0 - 4.0 %
Nickel, Ni 5.0 - 8.0 %5.0 - 8.0 %
Nitrogen, N 0.080 - 0.25 %0.080 - 0.25 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si <= 2.0 %<= 2.0 %
Sulfur, S <= 0.030 %<= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ATI Allegheny Ludlum Stainless Steel Type 201, 20% Cold Work (UNS S20100)
ATI Allegheny Ludlum Stainless Steel Type 201L, 10% Cold Work (UNS S20103)
ATI Allegheny Ludlum Stainless Steel Type 301, 1/2 Hard (UNS S30100)
Carpenter Pyrowear® 675 Stainless Steel, Tempered 316°C, Longitudinal Properties
Carpenter Pyrowear® 675 Stainless Steel, Tempered 316°C, Transverse Properties

MQCA872A30 / 13323

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.