MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chemours Krytox® XHT-SX PFPE Grease
Categories: Fluid; Lubricant; Perfluoropolyether (PFPE); PTFE Gellant

Material Notes: The Krytox® XHT-S and XHT-SX grease series is an extension of the Krytox® GPL 240 series and the Krytox® GPL 20X series, but the Krytox® XHT-S and XHT-SX greases are designed to give higher performance in the 204–302 °C (400–575 °F) ranges. The Krytox® XHT-S and XHT-SX greases should be used below 320 °C (608 °F), where the PTFE thickener could begin to melt. The base oil is an extremely viscous oil that provides good viscosity and lower evaporation at high temperatures. Krytox® XHT-S and XHT-SX greases contain no additives, so they are used where a potential for interaction between process chemicals and grease additives exists.

Chemours was formed from former DuPont performance chemicals businesses, including DuPont Performance Lubricants, in 2015.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.99 g/cc
@Temperature 0.000 °C
1.99 g/cc
@Temperature 32.0 °F
Volatiles <= 0.75 %
@Temperature 204 °C,
Time 79200 sec
<= 0.75 %
@Temperature 399 °F,
Time 22.0 hour
Viscosity Measurement 158158Base Oil Viscosity Index
Kinematic Viscosity 2610 cSt
@Temperature 20.0 °C
2610 cSt
@Temperature 68.0 °F
Base Oil
Kinematic Viscosity at 40°C (104°F) 738 cSt738 cStBase Oil
Kinematic Viscosity at 100°C (212°F) 65 cSt65 cStBase Oil
Vapor Pressure  <= 4.00e-17 bar
@Temperature 20.0 °C
<= 3.00e-14 torr
@Temperature 68.0 °F
 <= 1.33e-12 bar
@Temperature 100 °C
<= 1.00e-9 torr
@Temperature 212 °F
 <= 2.67e-9 bar
@Temperature 200 °C
<= 0.00000200 torr
@Temperature 392 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 300 °C572 °F
Minimum Service Temperature, Air <= -10.0 °C<= 14.0 °F
Pour Point <= -15.0 °C<= 5.00 °FBase Oil
 
Descriptive Properties
AppearanceWhite, creamy consistency
Food Contact ApprovalNSF H-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chemours Krytox® NRT 8904 PFPE Lubricant
Chemours Krytox® NRT 8906 PFPE Lubricant
Chemours Krytox® CORR 226 FG PFPE Corrugator Grease
Chemours Krytox® XHT-AC PFPE Grease
Chemours Krytox® XHT-BD Performance PFPE Lubricant

WDUPJ920 / 162454

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.