MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

BigRep PET-CF Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); PET + Carbon Fiber

Material Notes: BigRep's PET-CF is an engineering-grade filament for high-strength additive manufacturing applications. With exceptional dimensional stability and low moisture absorption, it's the perfect material for printing in industrial environments. Capable of producing exceptionally strong, sti_ parts with a fine surface finish and heat resistance up to 100 °C, this material is ideal for functional, performance applications. PET-CF is a reliable and easy to use materials for environments with limited control like a factory floor.

Highlights:

  • Strong and sti_ parts
  • High dimensional stability
  • Excellent surface finish
  • Heat resistant up to 100 °C
  • Low moisture absorption

Information provided by Bigrep

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³
Filament Diameter 2850 µm2850 µm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 100 MPa14500 psiISO 527
Flexural Modulus 8.00 GPa1160 ksiISO 178
Tensile Impact Strength 40.0 kJ/m²19.0 ft-lb/in²ISO 527
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) >= 100 °C>= 212 °FISO 75
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 200 - 220 °C392 - 428 °F
 
Descriptive Properties
Filament Net Weight2.5, 4.5 & 8.5 kg
Print Bed Temperature60°C
Printing Speed>40 mm/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBIGR009 / 250859

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.