MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

North American Red Alder Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Data is based on small, clear, air-dried samples unless specified.

Key Words: Alnus rubra; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.410 g/cc0.0148 lb/in³Air Dry (12-15% Moisture Content)
Cell Length 1.20 mm0.0472 inMature Wood
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 2600 N585 lb (f)Side
Tensile Strength, Ultimate 2.90 MPa421 psiPerpendicular to Grain
Modulus of Rupture 0.0380 GPa5.51 ksiStatic Bending
Flexural Modulus 9.50 GPa1380 ksiStatic Bending
Compressive Strength 3.00 MPa435 psiPerpendicular to Grain
 40.0 MPa5800 psiParallel to Grain
Shear Strength 7.40 MPa1070 psiOrientation Unknown
 
Thermal PropertiesMetricEnglishComments
Shrinkage 4.4 %4.4 %Radial; Green to Zero Moisture
 7.3 %7.3 %Tangential; Green to Zero Moisture
 12.6 %12.6 %Volumetric; Green to Zero Moisture

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
European Alder Wood
North American Black Willow Wood
American Red Maple Wood
North American Eastern Cottonwood Wood
North American Elm Wood

PTSA150 / 71253

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.