MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Encom Polymers EnTor PEI-10PF-BK PEI, Molding Grade, 10% PTFE
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: Appearance: Black

Processing Methods: Injection Molding, Profile Extrusion

Applications: Automotive, Electrical, Metallizable

UL File Number E175765

Information provided by EnCom Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.33 g/cc1.33 g/ccASTM D792
Filler Content 10 %10 %
Maximum Moisture Content 0.0200.020
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 98.0 MPa14200 psiASTM D638
Elongation at Break 20 %20 %ASTM D638
Flexural Modulus 3.079 GPa446.6 ksiASTM D790
Izod Impact, Notched 0.800 J/cm1.50 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 54.0 µm/m-°C30.0 µin/in-°FASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 199 °C390 °FASTM D648
Flammability, UL94  V-0
@Thickness 3.17 mm
V-0
@Thickness 0.125 in
 V-0
@Thickness 1.57 mm
V-0
@Thickness 0.0620 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 332 - 399 °C630 - 750 °F
Middle Barrel Temperature 338 - 399 °C640 - 750 °F
Front Barrel Temperature 343 - 399 °C650 - 750 °F
Nozzle Temperature 343 - 399 °C650 - 750 °F
Melt Temperature 349 - 399 °C660 - 750 °F
Mold Temperature 135 - 163 °C275 - 325 °F
Drying Temperature 149 °C300 °F
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hour
 <= 8.00 hour<= 8.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENCOM168 / 266182

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.