MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Overview of materials for AISI 8000 Series Steel
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 8000 Series Steel

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "AISI 8000 Series Steel". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.75 - 7.85 g/cc0.280 - 0.284 lb/in³Average value: 7.85 g/cc Grade Count:330
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 143 - 429143 - 429Average value: 276 Grade Count:295
Hardness, Knoop 169 - 682169 - 682Average value: 310 Grade Count:307
Hardness, Rockwell B 80.0 - 10580.0 - 105Average value: 97.2 Grade Count:272
Hardness, Rockwell C 10.0 - 64.010.0 - 64.0Average value: 31.1 Grade Count:257
Hardness, Vickers 155 - 661155 - 661Average value: 299 Grade Count:307
Tensile Strength, Ultimate 450 - 1520 MPa65300 - 221000 psiAverage value: 968 MPa Grade Count:265
Tensile Strength, Yield 240 - 1340 MPa34800 - 194000 psiAverage value: 756 MPa Grade Count:265
Elongation at Break 9.00 - 31.3 %9.00 - 31.3 %Average value: 18.6 % Grade Count:265
Reduction of Area 31.0 - 62.5 %31.0 - 62.5 %Average value: 53.6 % Grade Count:73
Modulus of Elasticity 187 - 210 GPa27100 - 30500 ksiAverage value: 205 GPa Grade Count:326
Bulk Modulus 160 - 170 GPa23200 - 24700 ksiAverage value: 160 GPa Grade Count:308
Poissons Ratio 0.270 - 0.3000.270 - 0.300Average value: 0.291 Grade Count:325
Fatigue Strength 205 - 485 MPa29700 - 70300 psiAverage value: 335 MPa Grade Count:6
Fracture Toughness 33.0 - 115 MPa-m½30.0 - 105 ksi-in½Average value: 67.3 MPa-m½ Grade Count:4
Machinability 55.0 - 70.0 %55.0 - 70.0 %Average value: 64.8 % Grade Count:304
Shear Modulus 72.0 - 82.0 GPa10400 - 11900 ksiAverage value: 79.9 GPa Grade Count:329
Izod Impact 14.0 - 115 J10.3 - 84.8 ft-lbAverage value: 65.1 J Grade Count:30
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000200 - 0.0000234 ohm-cm0.00000200 - 0.0000234 ohm-cmAverage value: 0.0000218 ohm-cm Grade Count:321
 
Thermal PropertiesMetricEnglishComments
CTE, linear 11.2 - 14.8 µm/m-°C6.22 - 8.22 µin/in-°FAverage value: 12.4 µm/m-°C Grade Count:103
Specific Heat Capacity 0.470 - 0.475 J/g-°C0.112 - 0.114 BTU/lb-°FAverage value: 0.475 J/g-°C Grade Count:305
Thermal Conductivity 37.6 - 52.0 W/m-K261 - 361 BTU-in/hr-ft²-°FAverage value: 46.6 W/m-K Grade Count:325
Transformation Temperature 397 - 828 °C747 - 1520 °FAverage value: 649 °C Grade Count:19
 
Component Elements PropertiesMetricEnglishComments
Boron, B 0.000500 - 0.00300 %0.000500 - 0.00300 %Average value: 0.00175 % Grade Count:35
Carbon, C 0.130 - 0.650 %0.130 - 0.650 %Average value: 0.311 % Grade Count:333
Chromium, Cr 0.300 - 1.00 %0.300 - 1.00 %Average value: 0.502 % Grade Count:332
Copper, Cu 0.000 - 0.250 %0.000 - 0.250 %Average value: 0.125 % Grade Count:3
Iron, Fe 96.1 - 99.1 %96.1 - 99.1 %Average value: 97.3 % Grade Count:333
Manganese, Mn 0.500 - 1.05 %0.500 - 1.05 %Average value: 0.825 % Grade Count:333
Molybdenum, Mo 0.0800 - 0.650 %0.0800 - 0.650 %Average value: 0.215 % Grade Count:333
Nickel, Ni 0.150 - 1.00 %0.150 - 1.00 %Average value: 0.549 % Grade Count:332
Phosphorus, P 0.000 - 0.0350 %0.000 - 0.0350 %Average value: 0.0340 % Grade Count:330
Silicon, Si 0.100 - 0.600 %0.100 - 0.600 %Average value: 0.237 % Grade Count:333
Sulfur, S 0.000 - 0.350 %0.000 - 0.350 %Average value: 0.0403 % Grade Count:330

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for AISI 4000 Series Steel
Overview of materials for AISI 5000 Series Steel
Overview of materials for AISI 9000 Series Steel
Overview of materials for Low Alloy Steel
Overview of materials for AISI 6000 Series Steel

M01003 / 81709

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.