MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Momentive Performance Materials PolarTherm® PT110 Boron Nitride (BN) Powder
Categories: Ceramic; Nitride; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Fine Hexagonal BN Powder

When used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic components and assemblies.

Information provided by Momentive Performance Materials, formerly GE Advanced Ceramics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.25 g/cc0.0813 lb/in³Theoretical
Particle Size 35 - 60 µm35 - 60 µmaverage
Specific Surface Area 0.10 - 1.0 m²/g0.10 - 1.0 m²/g
 
Mechanical PropertiesMetricEnglishComments
Hardness, Knoop 1111
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cm
Dielectric Constant 3.93.9
Dissipation Factor <= 0.00020
@Frequency 1e+6 Hz
<= 0.00020
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear <= 1.00 µm/m-°C
@Temperature 20.0 °C
<= 0.556 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 0.794 J/g-°C0.190 BTU/lb-°F
Thermal Conductivity 266 - 284 W/m-K1850 - 1970 BTU-in/hr-ft²-°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Corundum, Aluminum Oxide, Alumina, 99.9%, Al2O3
Alumina, alpha Al2O3, 99.5%
CeramTec V 679 Alumina, 99.7%
Materion BW 3250® High Thermal Conductivity 99.5% BeO
Silicon Carbide, Reaction-Bonded, SiSiC

CADV56 / 439

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.