MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

California Fine Wire Stablohm 812 Chromium, Aluminum, and Iron Resistance Wire
Categories: Metal; Electronic/Magnetic Alloy; Superalloy; Iron Base

Material Notes: All values may vary dependent on specific design and usage

Capabilities:

  • Wire
  • Ribbon
  • Square
  • Insulated
  • Plated

Information provided by California Fine Wire.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.25 g/cc0.262 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 793 MPa115000 psiAnnealed
 1210 MPa175000 psiStress relieved
 1380 MPa200000 psiHard
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000135 ohm-cm0.000135 ohm-cm3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
 
Thermal PropertiesMetricEnglishComments
CTE, linear 11.8 µm/m-°C
@Temperature 20.0 °C
6.56 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 0.460 J/g-°C
@Temperature 20.0 °C
0.110 BTU/lb-°F
@Temperature 68.0 °F
Thermal Conductivity 19.0 W/m-K132 BTU-in/hr-ft²-°F
Melting Point 1510 °C2750 °F
Maximum Service Temperature, Air 1177 °C2151 °FOperating Temperature
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 4.5 %4.5 %
Chromium, Cr 21 %21 %
Iron, Fe 74.5 %74.5 %as balance
 
Descriptive Properties
MagneticStrong
Temperature Coefficient of Resistance0.00002 ohms/ohm-°C0-100°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
GBC Cerasil™ 223U Ceramic
Du-Co Ceramics DC-16-L-3 Steatite
UBE Tyrannohex® Heat Resistant Composite
Boron Nitride, Cubic BN, (Borazone)
Crystex Composites Mykroy/Mycalex MM 800 Machining Grade Glass-bonded Mica Composite

NCALZ35 / 15578

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.