MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Celanese Celcon® GC25TF POM, 25% Glass Reinforced
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, 30% Glass Fiber Reinforced

Material Notes: Celcon« GC25TF is a 25% glass coupled acetal copolymer formulated for higher flow in thin walled and small parts. Celcon GC25TF is also exceptionally resistant to fuel. It offers excellent resistance to transportation fuels especially oxygenated fuels.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.58 g/cc1.58 g/ccASTM D792
Density 1.575 g/cc0.05690 lb/in³ISO 1183
Moisture Absorption 0.200 %0.200 %23°C/50%RH; ISO 62
Water Absorption at Saturation 0.80 %0.80 %ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.010 cm/cm0.010 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 120 MPa17400 psi5mm/min; ISO 527-2/1A
Tensile Strength, Yield 117 MPa17000 psiASTM D638
Elongation at Break 2.0 %2.0 %5mm/min; ISO 527-2/1A
 2.0 %2.0 %50mm/min; ISO 527-2/1A
Tensile Modulus 8.72 GPa1260 ksi50mm/min; ISO 527-2/1A
Flexural Modulus 8.27 GPa1200 ksiASTM D790
 8.71 GPa1260 ksiISO 178
Izod Impact, Notched 0.694 J/cm1.30 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 6.40 kJ/m²3.05 ft-lb/in²ISO 180/1A
Charpy Impact, Notched 0.640 J/cm²3.05 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 30.0 µm/m-°C16.7 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 100 µm/m-°C55.6 µin/in-°FISO 11359-2
Melting Point 165 °C329 °F10°C/min; ISO 11357-1,-2,-3
 166 °C331 °FASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 118 °C245 °FASTM D648
 162 °C324 °FISO 75-1, -2
 
Processing PropertiesMetricEnglishComments
Processing Temperature 90.0 - 120 °C194 - 248 °Fcavity
 190 - 210 °C374 - 410 °Fhot runner
Zone 1 170 - 180 °C338 - 356 °F
Zone 2 180 - 190 °C356 - 374 °F
Zone 3 180 - 190 °C356 - 374 °F
Zone 4 190 - 200 °C374 - 392 °F
Die Temperature 190 - 200 °C374 - 392 °F
Melt Temperature 180 - 200 °C356 - 392 °F
Drying Temperature 80.0 - 100 °C176 - 212 °F
Dry Time 3.00 hour3.00 hour
Injection Pressure 90.0 - 140 MPa13100 - 20300 psi
Hold Pressure 90.0 - 140 MPa13100 - 20300 psi
Back Pressure <= 2.00 MPa<= 290 psi
 
Descriptive Properties
Injection moldingYes
Injection speedslow
PelletsYes
Processing conditions acc. ISO9988-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Celcon® GC25A POM, 25% Glass Reinforced
Celanese Celcon® GC25T POM, 25% Glass Reinforced
Celanese Celcon® M90™ POM, Unfilled
Azoty Tarnow™ TARNOFORM 500 GF6 POM
Celanese Hostaform® C 9021 GV1/30 POM, 30% Glass Reinforced

PHCQ105 / 178560

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.