MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik VESTAMID® NRG 3001 PA 12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Extrusion/Tubing Grade

Material Notes: VESTAMID®NRG 3001 is a polyamide 12 compound developed for the manufacturing of hydrocarbon transport piping systems and liners. VESTAMID®NRG 3001 is characterized by easy processing and excellent dimensional control during pipe extrusion, especially by processing of large diameter pipes. The material has an excellent compatibility against hydrocarbons (i.e. crude oil) and oilfield chemicals (i.e. paraffin inhibitors) resulting in high dimensional stability and unaffected properties of parts in contact with those. The process temperature should be within a range of 220°C to 240°C. Generally, VESTAMID®NRG 3001 is processable on most of the commercially available PE extrusion machines. VESTAMID®NRG 3001 is supplied as cylindrical granules, ready for processing, in moisture-proof bags.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 38.0 MPa5510 psiISO 527
Elongation at Break >= 200 %>= 200 %ISO 527
Elongation at Yield 7.0 %7.0 %ISO 527
Tensile Modulus 1.32 GPa191 ksiISO 527
 0.259 GPa
@Temperature 100 °C
37.6 ksi
@Temperature 212 °F
after saturation in crude oil; ISO 527
 0.293 GPa
@Temperature 80.0 °C
42.5 ksi
@Temperature 176 °F
after saturation in crude oil; ISO 527
 0.336 GPa
@Temperature 60.0 °C
48.7 ksi
@Temperature 140 °F
after saturation in crude oil; ISO 527
 0.441 GPa
@Temperature 40.0 °C
64.0 ksi
@Temperature 104 °F
after saturation in crude oil; ISO 527
 0.770 GPa
@Temperature 23.0 °C
112 ksi
@Temperature 73.4 °F
after saturation in crude oil; ISO 527
Poissons Ratio  0.43
@Temperature 23.0 °C
0.43
@Temperature 73.4 °F
ISO 527
 0.45
@Temperature 100 °C
0.45
@Temperature 212 °F
ISO 527
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched  1.50 J/cm²
@Temperature -30.0 °C
7.14 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 5.40 J/cm²
@Temperature 23.0 °C
25.7 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear 252 µm/m-°C140 µin/in-°FISO 11359
Thermal Conductivity 0.240 W/m-K1.67 BTU-in/hr-ft²-°FASTM C177
Melting Point 176 °C349 °FISO 11357
 
Descriptive Properties
ColorNatural color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik VESTAMID® NRG 1001 PA 12
Evonik VESTAMID® NRG 6001 PA 12
Evonik VESTAMID® NRG 2101 PA 12
Evonik VESTAMID® NRG 2901 PA 12
Evonik VESTAMID® NRG 4101 PA 12

PEVONIL271 / 196475

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.