Orion Performance Compounds i-OnComp™ PSU GF30 Polysulfone, 30% Glass Fiber Reinforced
Categories:
Polymer
;
Thermoplastic
;
Polyphenylsulfone (PPSU)
;
Polyphenylsulfone, Glass or Carbon Fiber Reinforced
Material Notes:
18-103-000-000
Main Features:
High stiffness
Natural (beige) color
Target Industries:
Automotive
Oil and gas
Medical device enclosures
Information provided by Orion Performance Compounds, Inc.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.50
g/cc
1.50
g/cc
ASTM D792
Linear Mold Shrinkage, Flow
0.0030
-
0.0080
cm/cm
0.0030
-
0.0080
in/in
ASTM D955
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
123
MPa
17800
psi
ASTM D638
Tensile Strength, Yield
124
MPa
18000
psi
ASTM D638
Elongation at Break
1.6 %
1.6 %
ASTM D638
Tensile Modulus
7.79
GPa
1130
ksi
ASTM D638
Flexural Strength
179
MPa
26000
psi
ASTM D790
Flexural Modulus
6.96
GPa
1010
ksi
ASTM D790
Izod Impact, Notched
0.587
J/cm
1.10
ft-lb/in
ASTM D256
Electrical Properties
Metric
English
Comments
Volume Resistivity
>=
1.00e+12
ohm-cm
>=
1.00e+12
ohm-cm
ASTM D257
Surface Resistivity per Square
>=
1.00e+12
ohm
>=
1.00e+12
ohm
ASTM D257
Thermal Properties
Metric
English
Comments
Deflection Temperature at 0.46 MPa (66 psi)
189
°C
372
°F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
183
°C
361
°F
ASTM D648
Processing Properties
Metric
English
Comments
Nozzle Temperature
349
-
371
°C
660
-
700
°F
Zone 1
316
-
343
°C
600
-
650
°F
Zone 2
338
-
371
°C
640
-
700
°F
Zone 3
343
-
393
°C
650
-
740
°F
Melt Temperature
338
-
382
°C
640
-
720
°F
Mold Temperature
121
-
191
°C
250
-
375
°F
Drying Temperature
138
°C
280
°F
Dry Time
2.00
-
4.00
hour
2.00
-
4.00
hour
Moisture Content
<= 0.040 %
<= 0.040 %
Back Pressure
0.345
-
0.689
MPa
50.0
-
100
psi
Screw Speed
30
-
60
rpm
30
-
60
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PORI9992 / 318025
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.