MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Hostacom BE17FC BLK Polypropylene with 40% Calcium Carbonate (CaCO3) Filler
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 40% Calcium Carbonate (CaCO3) Filler

Material Notes: Hostacom BE17FC BLK fractional melt flow, 1,800 MPa flexural modulus, UV stabilized, precolored, 40% Calcium Carbonate filled polypropylene copolymer is typically used for a variety of extrusion and blow molding applications. It is characterized by an excellent overall balance of properties. Applications: Automotive Parts, Exterior Automotive Applications, Under hood.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³ASTM D792
Melt Flow 0.40 g/10 min
@Load 2.16 kg,
Temperature 230 °C
0.40 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8484ASTM D 785
Hardness, Shore D 7474ASTM D2240
Tensile Strength at Break 21.0 MPa3050 psi
Tensile Strength, Yield 27.0 MPa3920 psiASTM D638
Elongation at Break 280 %280 %ASTM D 638
Elongation at Yield 10 %10 %ASTM D 638
Flexural Modulus 1.80 GPa261 ksiASTM D790
Izod Impact, Notched 3.50 J/cm
@Temperature 23.0 °C
6.56 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Tear Strength 130 kN/m742 pliASTM D624
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 78.0 °C172 °Funannealed; ASTM D648
 
Descriptive Properties
Processing MethodExtrusion Blow Molding, Injection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Astryn BE17FC Polypropylene Copolymer, 40% Calcium Carbonate
Celanese SO.F.TER Polifor® 12 CA/40 40% Calcium Carbonate Reinforced Polypropylene
A. Schulman POLYFORT™ FPP 3707 CAC03 Filled Homopolymer Polypropylene
A. Schulman POLYFORT™ FPP 1245 CaCO3 Filled Copolymer Polypropylene
A. Schulman POLYFORT™ FPP 1200X High Flow, Calcium Carbonate Fortified Homopolymer Polypropylene

PEQT7675 / 219312

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.