Features and Typical Applications Primarily designed for ease of use in either meter mix or manual dispense operations. These products also offer a wide range of features including heat dissipation, thermal and mechanical shock resistance, and thermal conductivity.
Emerson & Cuming 2741LV/15LV Stycast® Two-Component Easy Mix Ratio Encapsulant
- Mix Ratio by weight = 400:100
- Good Chemical Resistance
Cure Type: Room Temp or Heat Bonding Type: Epoxy The Stycast® product line is now a part of Henkel; this specific grade is discontinued. |