MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mocom (ALBIS) ALCOM® POM 770/1 PTFE15 POM, 15% PTFE Reinforced
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, PTFE Filled

Material Notes: Base Polymer: Polyoxymethylene Copolymer

Filler/Additive System: 15% PTFE

Special Features: Improved sliding/wear

Market Segment: Automotive, Machinery

Application Area: Gear wheels, roller bearings

Typical Applications: Functional components, bearings and sliding elements

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.48 g/cc0.0535 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.020 - 0.024 cm/cm
@Time 86400 sec
0.020 - 0.024 in/in
@Time 24.0 hour
ISO 294-4
Linear Mold Shrinkage, Transverse 0.019 - 0.023 cm/cm
@Time 86400 sec
0.019 - 0.023 in/in
@Time 24.0 hour
ISO 294-4
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
6.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Storage Temperature <= 30.0 °C<= 86.0 °Fdry, protected from light
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 50.0 MPa7250 psiISO 527
Elongation at Break 11 %11 %ISO 527
Tensile Modulus 2.25 GPa326 ksiISO 527
Flexural Strength 60.0 MPa
@Strain 3.5 %
8700 psi
@Strain 3.5 %
ISO 178
Flexural Modulus 2.20 GPa319 ksiISO 178
Charpy Impact Unnotched  5.00 J/cm²
@Temperature 23.0 °C
23.8 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
 5.00 J/cm²
@Temperature -40.0 °C
23.8 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1eU
Charpy Impact, Notched  0.300 J/cm²
@Temperature 23.0 °C
1.43 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 0.350 J/cm²
@Temperature -40.0 °C
1.67 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 173 °C343 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C194 °FISO 75-1/-2
Vicat Softening Point 145 °C293 °FB50; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 220 °C356 - 428 °FInjection molding
Mold Temperature 60.0 - 100 °C140 - 212 °FInjection molding
Drying Temperature  100 - 110 °C
@Time 7200 - 10800 sec
212 - 230 °F
@Time 2.00 - 3.00 hour
in a dry air (desiccant) dryer
 100 - 110 °C
@Time 10800 - 18000 sec
212 - 230 °F
@Time 3.00 - 5.00 hour
in air circulating dryer
 
Descriptive Properties
Base PolymerPolyoxymethylene Copolymer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PALBIS8186 / 242245

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.