MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

AISI 1035 Steel, as cold drawn, 22-32 mm (0.875-1.25 in) round
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel; Medium Carbon Steel

Material Notes: Applications include levers, bolts, studs, nuts, and similar parts which are headed, upset, or extruded. Applications for wires include nails requiring high shank rigidity or strength and quench-hardened nails.

Key Words: UNS G10350, AMS 5080, AMS 5082, ASTM A29, ASTM A108, ASTM A510, ASTM A519, ASTM A544, ASTM A545, ASTM A546, ASTM A576, ASTM A682, FED QQ-S-635 (C1035), B.S. 080 A 37, B.S. 080 M 36, FED QQ-S-700 (C1035), SAE J403, SAE J412, SAE J414, DIN 1.0501, AFNOR CC 35 (France), UNI C 35, SS14 1550 (Sweden), B.S. 060 A 35, B.S. 080 A 32, B.S. 080 A 35
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.87 g/cc0.284 lb/in³Typical for steels.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 163163
Hardness, Knoop 184184Converted from Brinell
Hardness, Rockwell B 8484Converted from Brinell
Hardness, Vickers 170170Converted from Brinell
Tensile Strength, Ultimate 550 MPa79800 psi
Tensile Strength, Yield 485 MPa70300 psi
Elongation at Break 12 %12 %in 50 mm
Reduction of Area 35 %35 %
Modulus of Elasticity 196 GPa28400 ksi
Bulk Modulus 156 GPa22600 ksiEstimated from elastic modulus
Poissons Ratio 0.290.29Typical for steel
Shear Modulus 76.0 GPa11000 ksiEstimated from elastic modulus
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.0000163 ohm-cm
@Temperature 0.000 °C
0.0000163 ohm-cm
@Temperature 32.0 °F
annealed specimen
 0.0000217 ohm-cm
@Temperature 100 °C
0.0000217 ohm-cm
@Temperature 212 °F
annealed specimen
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.0 µm/m-°C
@Temperature 20.0 - 100 °C
6.11 µin/in-°F
@Temperature 68.0 - 212 °F
 11.9 µm/m-°C
@Temperature 20.0 - 200 °C
6.61 µin/in-°F
@Temperature 68.0 - 392 °F
 13.9 µm/m-°C
@Temperature 20.0 - 500 °C
7.72 µin/in-°F
@Temperature 68.0 - 932 °F
 14.4 µm/m-°C
@Temperature 20.0 - 600 °C
8.00 µin/in-°F
@Temperature 68.0 - 1110 °F
 14.8 µm/m-°C
@Temperature 20.0 - 700 °C
8.22 µin/in-°F
@Temperature 68.0 - 1290 °F
Specific Heat Capacity 0.486 J/g-°C
@Temperature >=100 °C
0.116 BTU/lb-°F
@Temperature >=212 °F
annealed
Thermal Conductivity  43.6 W/m-K
@Temperature 100 °C
303 BTU-in/hr-ft²-°F
@Temperature 212 °F
Estimated
 50.7 W/m-K
@Temperature 0.000 °C
352 BTU-in/hr-ft²-°F
@Temperature 32.0 °F
Estimated
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.31 - 0.38 %0.31 - 0.38 %
Iron, Fe 98.63 - 99.09 %98.63 - 99.09 %As remainder
Manganese, Mn 0.60 - 0.90 %0.60 - 0.90 %
Phosphorus, P <= 0.040 %<= 0.040 %
Sulfur, S <= 0.050 %<= 0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1035 Steel, as cold drawn, 16-22 mm (0.625-0.875 in) round
AISI 1035 Steel, as cold drawn, 32-50 mm (1.25-2 in) round
AISI 1035 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1035 Steel, as cold drawn, 50-75 mm (2-3 in) round
AISI 1035 Steel, as rolled, 19-32 mm (0.75-1.25 in) round

M1035F / 6918

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.