MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mitsui AURUM® PL6200 Thermoplastic Polyimide Resin, Non-filled  (discontinued **)
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic; Thermoplastic Polyimide, Unfilled

Material Notes: Usable at up to 240°C. Satisfactory sliding properties. A low, stable coefficient of friction and low friction wear. Outstanding dimensional stability. Stable coefficient of expansion and satisfactory creep characteristics. Exceptionally clean properties. Trace amounts of outgas and metallic impurities.

Applications: Precision machinery, industrial machinery parts, electrical and electronic parts, automotive and transport equipment parts, special insulation, metal alternative, film, fiber, matrix composite materials, HDD parts and semiconductor manufacturing equipment, copier machine parts

Typical property data for non-crystallized parts is reported here. Recommended Condition for Crystallization = 220°C X 5hrs + 280°C X 5hrs.

Information provided by Mitsui.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.31 g/cc0.0473 lb/in³ASTM D792
Linear Mold Shrinkage, Flow 0.0090 cm/cm0.0090 in/in
Linear Mold Shrinkage, Transverse 0.014 cm/cm0.014 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 91.0 MPa13200 psiASTM D638
Elongation at Break 56 %56 %ASTM D638
Flexural Strength 138 MPa20000 psiASTM D790
Flexural Modulus 3.10 GPa450 ksiASTM D790
Izod Impact, Notched 0.900 J/cm1.69 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 240 °C464 °F
Glass Transition Temp, Tg 250 °C482 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ensinger Sintimid™ V Unfilled Polyimide (PI)
Mitsui AURUM® 450 Thermoplastic Polyimide Resin, Non-filled
DuPont Mobility and Materials VESPEL TP-8054 Polyimide
DuPont™ Kapton® 500VN Polyimide Film, 125 Micron Thickness
DuPont Mobility and Materials Vespel® SP-1 Polyimide, Machined

PMIT045Em / 222920

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.