MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

EVALCA EVAL® EP-J102B Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Alcohol (EVOH)

Material Notes: 32 mol % Ethylene.

Data provided by EVALCA. Designed to provide a wide thermoforming range together with high barrier properties. EVAL® EP-J102B is specifically designed for thermoforming applications using polystyrene and polyethylene structural layers. This resin can be used with SPPF or melt phase forming techniques. EVOH is used in packaging applications because of its outstanding gas barrier properties.

EVAL™ is now produced as a part of the Kuraray product line.

Key Words: Ethylene Vinylalcohol
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0423 lb/in³ASTM D1505
Moisture Vapor Transmission 1.50 cc-mm/m²-24hr-atm3.81 cc-mil/100 in²-24hr-atm40°C, 90% RH
Oxygen Transmission 0.0120 cc-mm/m²-24hr-atm0.0305 cc-mil/100 in²-24hr-atm20°C; 65% RH; Permeability increases significantly at higher moisture content.
Melt Flow  2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 4.9 g/10 min
@Load 2.16 kg,
Temperature 210 °C
4.9 g/10 min
@Load 4.76 lb,
Temperature 410 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9595Estimated by MatWeb from similar grades
Tensile Strength, Yield 69.0 MPa10000 psiEstimated by MatWeb from similar grades
Film Elongation at Break, MD 270 %270 %Orientation not specified; ASTM D882
Modulus of Elasticity 2.00 GPa290 ksiEstimated by MatWeb from similar grades
Film Tensile Strength at Break, MD 57.0 MPa8270 psiOrientation not specified; ASTM D882
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 5.55.5Frequency Not Specified
Dissipation Factor 0.210.21Frequency Not Specified
 
Thermal PropertiesMetricEnglishComments
CTE, linear  65.0 µm/m-°C
@Temperature 20.0 °C
36.1 µin/in-°F
@Temperature 68.0 °F
Estimated by MatWeb from similar grades
 120 µm/m-°C
@Temperature 100 °C
66.7 µin/in-°F
@Temperature 212 °F
Estimated by MatWeb from similar grades
Specific Heat Capacity 2.40 J/g-°C0.574 BTU/lb-°FEstimated by MatWeb from similar grades
Thermal Conductivity 0.340 W/m-K2.36 BTU-in/hr-ft²-°FFor EVAL F101
Melting Point 183 °C361 °FDSC
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C194 °FFor EP-H101
Vicat Softening Point 165 °C329 °FFor EP-H101
Glass Transition Temp, Tg 69.0 °C156 °FDynamic Viscoelasticity
 
Optical PropertiesMetricEnglishComments
Haze 1.9 %1.9 %Film; ASTM D1003
Gloss 85 %85 %45°; Film; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Processing Temperature 215 °C419 °FDie temperature

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EVALCA EVAL® LC-T101 Ethylene Vinyl Alcohol Copolymer Resin
EVALCA EVAL® LC-L101A Ethylene Vinyl Alcohol Copolymer Resin
EVALCA EVAL® LC-F101BZ Ethylene Vinyl Alcohol Copolymer Resin
EVALCA EVAL® F100 Ethylene Vinyl Alcohol Copolymer Resin
EVALCA EVAL® EP-F104BW Ethylene Vinyl Alcohol Copolymer Resin

PEVAL5 / 37295

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.