MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Trinseo Plexiglas® DR® M2 Acrylic
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Impact Modified, Molded

Material Notes: Plexiglas® DR® M2 is an impact modified thermoplastic acrylic resin formulated for injection molding and extrusion applications. It has a matte appearance, is heat resistance and provides 10 times the impact resistance of standard acrylics. It offers an excellent balance between melt flow and increased resistance to breakage, while providing weatherability superior to that provided by other high-impact plastics.

Appearance: Matte Finish; Clear/Transparent

Characteristics: Scratch Resistant; Good Dimensional Stability; Low Shrinkage; Good Thermal Stability; Good UV Resistance; Good Weather Resistance; Good Toughness; High Impact Resistance

Arkema has sold the American Plexiglas® product line to Trinseo, finalized in 2021.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/ccASTM D792
Melt Flow 1.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
1.0 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Izod Impact, Notched 0.427 J/cm0.800 ft-lb/inASTM D256
 
Optical PropertiesMetricEnglishComments
Haze 2.5 %
@Thickness 3.17 mm
2.5 %
@Thickness 0.125 in
ASTM D1003
Transmission, Visible 88 %
@Thickness 3.17 mm
88 %
@Thickness 0.125 in
ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type A2 Tool Steel
Overview of materials for Acrylic, Impact Modified, Molded
Bohler-Uddeholm AISI A2 Cold Work Tool Steel
Bhansali Engineering Abstron IM17SHG PMMA- ABS Alloy
ATI Allegheny Ludlum M2 Tool Steel, UNS T11302

PARKG044d / 108349

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.