MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

A. Schulman POLYFLAM™ FPP 1007E Talc Filled Homopolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 40% Talc Filler

Material Notes: Description

Polyfort® FPP 1007E is a 40% talc filled homopolymer compound for extrusion applications.

Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Melt Flow 2.0 g/10 min2.0 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 34.0 MPa4930 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
Flexural Strength 62.0 MPa8990 psiASTM D790
Flexural Modulus 3.31 GPa480 ksiASTM D790
Izod Impact, Notched 0.320 J/cm0.599 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 130 °C266 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C176 °FASTM D648
UL RTI, Electrical  120 °C
@Thickness 0.780 mm
248 °F
@Thickness 0.0307 in
UL 746
 120 °C
@Thickness 1.57 mm
248 °F
@Thickness 0.0618 in
UL 746
 120 °C
@Thickness 3.17 mm
248 °F
@Thickness 0.125 in
UL 746
UL RTI, Mechanical with Impact  115 °C
@Thickness 0.780 mm
239 °F
@Thickness 0.0307 in
UL 746
 115 °C
@Thickness 1.57 mm
239 °F
@Thickness 0.0618 in
UL 746
 115 °C
@Thickness 3.17 mm
239 °F
@Thickness 0.125 in
UL 746
UL RTI, Mechanical without Impact  115 °C
@Thickness 0.780 - 1.57 mm
239 °F
@Thickness 0.0307 - 0.0618 in
UL 746
 120 °C
@Thickness 3.17 mm
248 °F
@Thickness 0.125 in
UL 746
Flammability, UL94  HB
@Thickness 0.780 mm
HB
@Thickness 0.0307 in
 HB
@Thickness 1.57 mm
HB
@Thickness 0.0618 in
 HB
@Thickness 3.17 mm
HB
@Thickness 0.125 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman POLYFLAM™ FPP 1007 Talc Filled Homopolymer Polypropylene
A. Schulman POLYFLAM™ FPP 1007F Talc Filled Homopolymer Polypropylene
A. Schulman POLYFORT™ FPP 1007X Extra High Flow, Talc Fortified Homopolymer Polypropylene
A. Schulman POLYFORT™ FPP 2122UV-M-31 Black, Talc Filled Copolymer Polypropylene
A. Schulman POLYFORT™ FPP 3717 Talc Filled Homopolymer Polypropylene (39.6% Mineral Content)

PASHU112 / 25076

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.