MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Henkel Loctite® Stycast® 2651MM with CAT 11 Two-Component General Purpose Encapsulant
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Designed as a general purpose encapsulant which requires low viscosity and low abrasion. It is especially useful for machine dispensing and for parts that require post molding machining.

2651MM is a filled, low viscosity, general purpose, epoxy encapsulant. It contains a soft filler that both reduces abrasion in meter/mix equipment and enhances machinability in the cured product. Property data reported for 2651MM with CAT 11 Catalyst.

  • Good Chemical Resistance
  • Filled
  • High temperature
  • Thermally conductive
  • Mix Ratio by Weight = 100:8.5
Cure Type: Heat

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.59 g/cc0.0574 lb/in³Mixed
 1.61 g/cc0.0582 lb/in³Part A, 2651MM
Water Absorption 0.10 %
@Time 86400 sec
0.10 %
@Time 24.0 hour
Boil, Cured
Viscosity 48 cP
@Temperature 65.0 °C
48 cP
@Temperature 149 °F
Part B, CAT 11
Brookfield Viscosity 13000 cP13000 cPMixed
 35000 cP35000 cPPart A, 2651MM; Spindle 5, speed 5 rpm
Linear Mold Shrinkage 0.0020 cm/cm0.0020 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D <= 89<= 89
Tensile Strength 48.0 MPa6960 psi
Flexural Strength 83.0 MPa12000 psi
Compressive Strength 104 MPa15100 psi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  7.00e+12 ohm-cm
@Temperature 150 °C
7.00e+12 ohm-cm
@Temperature 302 °F
 4.00e+14 ohm-cm
@Temperature 25.0 °C
4.00e+14 ohm-cm
@Temperature 77.0 °F
Dielectric Constant  3.7
@Frequency 1e+6 Hz
3.7
@Frequency 1e+6 Hz
 4.4
@Frequency 1000 Hz
4.4
@Frequency 1000 Hz
 4.6
@Frequency 60 Hz
4.6
@Frequency 60 Hz
Dielectric Strength 17.7 kV/mm450 kV/in
Dissipation Factor  0.010
@Frequency 1000 Hz
0.010
@Frequency 1000 Hz
 0.020
@Frequency 60 Hz
0.020
@Frequency 60 Hz
 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 40.0 µm/m-°C22.2 µin/in-°FTMA
Thermal Conductivity 0.600 W/m-K4.16 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 155 °C311 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  30.0 - 60.0 min
@Temperature 120 °C
0.500 - 1.00 hour
@Temperature 248 °F
Option 3
 120 - 240 min
@Temperature 100 °C
2.00 - 4.00 hour
@Temperature 212 °F
Option 2
 480 - 960 min
@Temperature 80.0 °C
8.00 - 16.0 hour
@Temperature 176 °F
Option 1
Working Life >= 240 min
@Temperature 25.0 °C
>= 240 min
@Temperature 77.0 °F
100 g
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
AppearanceBlackCured
Mix Ratio, by Volume100 : 13Material : Catalyst
Mix Ratio, by Weight100 : 8.5Material : Catalyst

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler

PEMERS43 / 35735

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.