MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chemours Teflon™ PFA 945HP Plus Premium fluoroplastic resin
Categories: Polymer; Thermoplastic; Fluoropolymer; Perfluoroalkoxy (PFA); Polyperfluoroalkoxyethylene, Molded/Extruded

Material Notes: Teflon™ PFA 945HP Plus is a premium fluoroplastic resin available in pellet form. Teflon™ PFA 945HP Plus possesses the same exceptional chemical resistance, high purity, and protection against ionic contamination as Teflon™ PFA HP grades with the added benefits of improved flex life (typical MIT flex of 800,000*) and chemical stress-crack resistance. Teflon™ PFA 945HP Plus meets the increasingly stringent requirements for ultra-reliable and non-contaminating parts, as well as unmatched HCl permeation resistance. The improved flex life and chemical resistance will reduce the cost of ownership of high purity fluid handling systems by reducing downtime caused by mechanical or chemical stresses. Additionally, parts molded with Teflon™ PFA 945HP Plus have improved clarity and a smooth finish, which can further help prevent buildup of microbial contamination in water handling systems. With a typical MIT folding endurance of 800,000* cycles, Teflon™ PFA 945HP Plus is designed to withstand repeated flexing and aggressive chemical stress-cracking agents. Applications for Teflon™ PFA 945HP Plus include fluid handling components for high-performance chemical delivery systems, as well as tubing, unsupported pipe linings for the production of ultra-pure chemicals, and semiconductor components where purity in the parts-per-billion range is critical.

Information provided by Chemours.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.15 g/cc2.15 g/ccASTM D792
Water Absorption <= 0.030 %
@Time 86400 sec
<= 0.030 %
@Time 24.0 hour
ASTM D570
Melt Flow 7.0 g/10 min7.0 g/10 minASTM D3307
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5555ASTM D2240
Tensile Strength  13.0 MPa
@Temperature 200 °C
1890 psi
@Temperature 392 °F
ASTM D3307
 28.0 MPa
@Temperature 23.0 °C
4060 psi
@Temperature 73.4 °F
ASTM D3307
Elongation, Ultimate  290 %
@Temperature 23.0 °C
290 %
@Temperature 73.4 °F
ASTM D3307
 450 %
@Temperature 200 °C
450 %
@Temperature 392 °F
ASTM D3307
Flexural Modulus  0.0550 GPa
@Temperature 200 °C
7.98 ksi
@Temperature 392 °F
ASTM D790
 0.600 GPa
@Temperature 23.0 °C
87.0 ksi
@Temperature 73.4 °F
ASTM D790
Flex Crack Resistance 800000
@Thickness 0.203 mm
800000
@Thickness 0.00800 in
Cycles MIT Folding Endurance; ASTM D2176
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+18 ohm-cm>= 1.00e+18 ohm-cmASTM D257
Surface Resistivity per Square >= 1.00e+17 ohm>= 1.00e+17 ohmASTM D257
Dielectric Constant 2.03
@Frequency 1e+6 Hz
2.03
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 80.0 kV/mm
@Thickness 0.250 mm
2030 kV/in
@Thickness 0.00984 in
Short Time; ASTM D149
Dissipation Factor 0.00020
@Frequency 1e+6 Hz
0.00020
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance >= 180 sec>= 180 secASTM D495
 
Thermal PropertiesMetricEnglishComments
Melting Point 290 °C554 °FASTM D4591
Flammability, UL94 V-0V-0
Oxygen Index >= 95 %>= 95 %ASTM D2863
 
Descriptive Properties
Chemical/Solvent ResistanceExcellentASTM D543
Critical Shear Rate (1/s)21372°C
Heat of Combustion5.3 MJ/kgASTM D240
Salt Spray Resistance Coatings (hours)1000ASTM B117. 5% NaCl at 35 °C (95 °F).
Weather and Chemical ResistanceOutstanding
Weather Resistance (years unaffected)10Florida Exposure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDU8808 / 268734

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.