MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Master Bond EP62-1LO Two Component Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive; Epoxy, High Temperature

Material Notes: Key Features:
  • Very high glass transition temperature
  • Meets NASA low outgassing specifications
  • Exceptionally long working life at room temperature
  • Superior bond strength properties
Product Description: Master Bond EP62-1LO is a two component epoxy system that has an exceptionally long working life at ambient temperatures and cures rapidly at moderately elevated temperatures. It has a very forgiving 100 to 10 mix ratio by weight. The pot life of 100 grams is greater than 12 hours. Typical cure schedules range from 4-6 hours at 60-70°C, 20-40 minutes at 80-100°C or 10 minutes at 125°C. The cured epoxy resin exhibits remarkably high thermal stability with a glass transition temperature exceeding 170°C. Also noteworthy is its outstanding chemical resistance to acids, bases, many solvents and other chemicals, even at elevated temperatures (as listed in the table below). This system has excellent electrical insulation properties. The color of Part A is clear and Part B is dark brown in color. EP62-1LO is primarily used as an adhesive, sealant and coating where the epoxy will be exposed to very aggressive conditions as well as where a long open time and NASA low outgassing are required.

Product Advantages:

  • Easy to use, very forgiving 100 to 10 mix ratio by weight (will fully cure using 100 to 5 mix ratio)
  • Exceptionally long working life
  • Superior resistance to a wide variety of chemicals, even at high temperatures
  • Superb electrical insulation properties
  • Service temperature range of -60°F to +450°F
  • Versatile cure schedules at various elevated temperatures
  • Outstanding dimensional stability
  • Excellent physical strength properties
  • Meets NASA low outgassing standards

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Viscosity 100 - 1000 cP100 - 1000 cPPart B
 4000 - 8000 cP4000 - 8000 cPmixed
 10000 - 14000 cP10000 - 14000 cPPart A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D >= 80>= 80
Tensile Strength >= 58.6 MPa>= 8500 psi
Elongation at Break <= 2.0 %<= 2.0 %
Tensile Modulus 3.45 - 3.79 GPa500 - 550 ksi
Adhesive Bond Strength >= 15.9 MPa>= 2300 psiTensile lap, Aluminum to Aluminum
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cm
Dielectric Constant 3.25
@Frequency 60 Hz
3.25
@Frequency 60 Hz
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 232 °C450 °F
Minimum Service Temperature, Air -51.1 °C-60.0 °F
Glass Transition Temp, Tg >= 170 °C>= 338 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  10.0 min
@Temperature 125 °C
0.167 hour
@Temperature 257 °F
 20.0 - 40.0 min
@Temperature 80.0 - 100 °C
0.333 - 0.667 hour
@Temperature 176 - 212 °F
 240 - 360 min
@Temperature 60.0 - 70.0 °C
4.00 - 6.00 hour
@Temperature 140 - 158 °F
Working Life >= 720 min>= 720 minAfter mixing, 100 g batch
Shelf Life 12.0 Month12.0 Monthin original, unopened containers
 
Descriptive Properties
Chemical ResistanceAmmonium hydroxideResistant at 180°F, Immersion >30 Days
 Distilled waterResistant at 180°F, Immersion >30 Days
 EthanolResistant at 180°F, Immersion >30 Days
 Ethyl acetateResistant at 180°F, Immersion >30 Days
 Hydrochloric acid (10%)Resistant at 180°F, Immersion >30 Days
 Hydrogen peroxide (99%)Resistant at 180°F, Immersion >30 Days
 Jet fuelResistant at 180°F, Immersion >30 Days
 MEKResistant at 180°F, Immersion >30 Days
 MethanolResistant at 180°F, Immersion >30 Days
 Phosphoric acid (50%)Resistant at 180°F, Immersion >30 Days
 Potassium hydroxide (50%)Resistant at 180°F, Immersion >30 Days
 Sodium chloride (50%)Resistant at 180°F, Immersion >30 Days
 Sodium hydroxide (50%)Resistant at 180°F, Immersion >30 Days
 Sulfuric acid (10%)Resistant at 180°F, Immersion >30 Days
 Sulfuric acid (70%)Resistant at 180°F, Immersion >30 Days
 TolueneResistant at 180°F, Immersion >30 Days
Mixing Ratio100:10 by weightParts A to B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond Supreme 42HT-2ND-2 Two Component Epoxy
Master Bond Supreme 42HT-2ND Two Component Epoxy
Master Bond Supreme 12AOHT-LO One Component Epoxy
Master Bond EP62-1 High Glass Transition Temperature Epoxy System
Master Bond EP46HT-2ND2 Two Part Epoxy

PMASTM895 / 185488

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.