MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mocom (ALBIS) ALCOM® LDDC PMMA 1000 UV 18123 BK1016-11 PMMA, UV stabilized
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, UV Stabilized, Molded

Material Notes: Base Polymer: Polymehtylmethacrylate

Filler/Additive System: UV stabilized

Special Features: translucent

Market Segment: Automotive, Lighting

Application Area: Interior decoration/finishing, light transparent components, Black Panel-Technology

Typical Applications: lamp covers, display elements, operating elements

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³ISO 1183
Melt Flow 5.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
5.0 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 80.0 MPa11600 psiISO 527
Elongation at Break 3.0 %3.0 %ISO 527
Tensile Modulus 3.40 GPa493 ksiISO 527
Flexural Strength 110 MPa16000 psiISO 178
Flexural Modulus 3.50 GPa508 ksiISO 178
Charpy Impact Unnotched  2.00 J/cm²
@Temperature -20.0 °C
9.52 ft-lb/in²
@Temperature -4.00 °F
ISO 179/1eU
 2.00 J/cm²
@Temperature -40.0 °C
9.52 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1eU
 2.50 J/cm²
@Temperature 23.0 °C
11.9 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C203 °FISO 75-1/-2
Vicat Softening Point 110 °C230 °FB50; ISO 306
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
Glow Wire Flammability Index  650 °C
@Thickness 1.00 mm
1200 °F
@Thickness 0.0394 in
passed; DIN EN 60695
 650 °C
@Thickness 2.00 mm
1200 °F
@Thickness 0.0787 in
passed; DIN EN 60695
 650 °C
@Thickness 3.00 mm
1200 °F
@Thickness 0.118 in
passed; DIN EN 60695
 650 °C
@Thickness 4.00 mm
1200 °F
@Thickness 0.157 in
passed; DIN EN 60695
 
Optical PropertiesMetricEnglishComments
Haze 11 %
@Thickness 1.00 mm
11 %
@Thickness 0.0394 in
A,2°; ISO 13468
Transmission, Visible 34.5 %
@Thickness 1.00 mm
34.5 %
@Thickness 0.0394 in
A,2°; ISO 13468
 
Processing PropertiesMetricEnglishComments
Melt Temperature 210 - 280 °C410 - 536 °FInjection molding
Mold Temperature 50.0 - 80.0 °C122 - 176 °FInjection molding
Drying Temperature  65.0 - 90.0 °C
@Time 10800 - 14400 sec
149 - 194 °F
@Time 3.00 - 4.00 hour
in a dry air (desiccant) dryer
 65.0 - 90.0 °C
@Time 14400 - 21600 sec
149 - 194 °F
@Time 4.00 - 6.00 hour
in air circulating dryer
 
Descriptive Properties
Base PolymerPolymehtylmethacrylate
Half Power Angled=1mm, A,2°

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Altuglas® 84 L Acrylic-Styrene Copolymer
European Oak Wood
ESK Ceramics PolyCeram® TRIBO140 Polymer matrix composite
Trinseo Plexiglas® V045 Acrylic
Plaskolite West Optix® CA-41 General Purpose Acrylic Resin

PALBIS8074 / 242133

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.