MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AdvanSix Capran® 996 Heat Stabilized Nylon Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Film Grade

Material Notes: Description: Capran® 996 is a blue tinted, heat-stabilized cast film produced from modified nylon resin. Capran® 996 has excellent heat stability and resistance to pinholing. It can be used at temperatures up to 450°F (232°C) for typical cure cycle times.

Applications: Capran® 996 is recommended as bagging film for advanced composite fabrication and other high temperature applications where softness and workability are essential.

Former Honeywell product; AdvanSix is a spin-off of Honeywell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0410 lb/in³Yield Density
Thickness 50.8 microns2.00 mil
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 76.0 MPa11000 psiASTM D882
Tensile Strength, Yield 66.0 MPa9570 psiASTM D882
Elongation at Break 300 %300 %ASTM D882
Tear Strength Test 3030grams/mil; ASTM D1922
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °Fcrystalline melting point; Hot Stage Microscope
Shrinkage <= 1.0 %
@Temperature 149 °C,
Time 1800 sec
<= 1.0 %
@Temperature 300 °F,
Time 0.500 hour
ASTM D1204

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® 8234G HS 44% Glass Filled PA6 (Dry)
BASF Ultramid® 8234G HS 44% Glass Filled PA6 (Conditioned)
BASF Ultramid® 8233G HS BK-106 33% Glass Filled PA6 (Dry)
BASF Petra® 140 45% Glass Filled PET
BASF Capron® 8232G 25% Glass-Filled Nylon 6 (Conditioned)

PALC020 / 23781

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.