Good weldability/formability and very good corrosion resistance lead to applications such as food and chemical handling, tanks, trim, litho sheet, pressure vessels, and piping. Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN. Composition Notes: Composition information provided by the Aluminum Association and is not for design. |
UNS A93003; ISO AlMn1Cu; Aluminium 3003-H16; AA3003-H16; Al3003-H16 |