MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Epoxyset Epoxiohm EO-24 Electrically Conductive Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, Electrically Conductive

Material Notes: EO-24 is a two components, 100% solids silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is used for thermal management applications due to its high thermal conductivity.

Information provided by Epoxyset Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.10 g/cc0.112 lb/in³
Viscosity 3000 cP3000 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585ASTM D2240
Shear Strength 23.0 MPa3340 psi
Adhesive Bond Strength 9.65 MPa1400 psiLap Shear Strength
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity <= 0.000400 ohm-cm<= 0.000400 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 30.0 µm/m-°C16.7 µin/in-°F
Thermal Conductivity >= 2.50 W/m-K>= 17.4 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 200 °C392 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
Glass Transition Temp, Tg 88.0 °C190 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  5.00 min
@Temperature 175 °C
0.0833 hour
@Temperature 347 °F
 60.0 min
@Temperature 125 °C
1.00 hour
@Temperature 257 °F
Pot Life >= 480 min>= 480 min

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEPOXY814 / 150839

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.