MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

85% Alumina, vitreous body
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Fair Thermal Shock resistance, Tc value = 750-1000°C (1380-1830°F).

Key Words: aluminum oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.40 - 3.53 g/cc0.123 - 0.128 lb/in³
Water Absorption 0.00 - 0.020 %0.00 - 0.020 %24 hrs.
Open Porosity <= 1.0 %<= 1.0 %Hermetic (helium mass spectrometer test on 0.254 mm (0.010 in) sections)
 
Mechanical PropertiesMetricEnglishComments
Knoop Microhardness 14501450
Hardness, Mohs 8.5 - 9.08.5 - 9.0
Tensile Strength, Ultimate 115 - 160 MPa16700 - 23200 psi
Modulus of Elasticity 215 - 240 GPa31200 - 34800 ksi
Flexural Strength 205 - 310 MPa29700 - 45000 psi
Compressive Strength 965 - 2760 MPa140000 - 400000 psi
Charpy Impact 0.660 - 0.790 J0.487 - 0.583 ft-lb
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  400000 - 500000 ohm-cm
@Temperature 900 °C
400000 - 500000 ohm-cm
@Temperature 1650 °F
 1.00e+8 - 7.50e+9 ohm-cm
@Temperature 500 °C
1.00e+8 - 7.50e+9 ohm-cm
@Temperature 932 °F
 2.00e+13 - 7.50e+13 ohm-cm
@Temperature 100 °C
2.00e+13 - 7.50e+13 ohm-cm
@Temperature 212 °F
 1.00e+14 - 3.60e+14 ohm-cm
@Temperature 25.0 °C
1.00e+14 - 3.60e+14 ohm-cm
@Temperature 77.0 °F
Dielectric Strength 8.07 - 13.8 kV/mm205 - 351 kV/inAC
 
Thermal PropertiesMetricEnglishComments
CTE, linear  5.47 - 5.68 µm/m-°C
@Temperature 25.0 - 200 °C
3.04 - 3.16 µin/in-°F
@Temperature 77.0 - 392 °F
 6.55 - 6.96 µm/m-°C
@Temperature 25.0 - 600 °C
3.64 - 3.87 µin/in-°F
@Temperature 77.0 - 1110 °F
 7.33 µm/m-°C
@Temperature 25.0 - 800 °C
4.07 µin/in-°F
@Temperature 77.0 - 1470 °F
 7.60 - 7.90 µm/m-°C
@Temperature 25.0 - 700 °C
4.22 - 4.39 µin/in-°F
@Temperature 77.0 - 1290 °F
 7.67 - 7.89 µm/m-°C
@Temperature 25.0 - 1000 °C
4.26 - 4.38 µin/in-°F
@Temperature 77.0 - 1830 °F
Specific Heat Capacity 0.419 J/g-°C0.100 BTU/lb-°F
Thermal Conductivity  13.0 - 17.0 W/m-K
@Temperature 38.0 °C
90.2 - 118 BTU-in/hr-ft²-°F
@Temperature 100 °F
 26.0 W/m-K
@Temperature 425 °C
180 BTU-in/hr-ft²-°F
@Temperature 797 °F
 33.0 W/m-K
@Temperature 870 °C
229 BTU-in/hr-ft²-°F
@Temperature 1600 °F
Maximum Service Temperature, Air 1200 - 1400 °C2190 - 2550 °Fmaximum working temperature
 
Component Elements PropertiesMetricEnglishComments
Al2O3 85 %85 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
95% Alumina, vitreous body
Corundum, Aluminum Oxide, Alumina, 99.9%, Al2O3
99.5% Alumina, vitreous body
92% Alumina, opaque
96% Alumina, thick-film, as fired

BA2C / 137

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.