MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AGC Fluon® AH-3000 LM-ETFE, Conductive Type, Fluororesin
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE; Modified ETFE, Unreinforced

Material Notes: Fluon®LM-ETFE AH series is a fluoro-resin which have an adhesive properties, and is possible to adhere with other materials by melting down. It can be applied directly without privilege adhesive agent or surface treatment that is used at previous system. Excellent adhesiveness of the two-layer system is effected for only one step. Furthermore, the conventional properties such as anti stick, excellent moldability and chemical resistance, are same as conventional fluoro-resin.

Information provided by Asahi Glass Company, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.80 g/cc1.80 g/ccASTM D792
Melt Flow 25 g/10 min25 g/10 minASTM D359
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 35.0 MPa5080 psiASTM D638
Elongation at Break 350 %350 %ASTM D638
Flexural Modulus 1.24 GPa180 ksiASTM D790
Izod Impact, Notched NBNBASTM D256
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 1000 ohm1000 ohm
 
Thermal PropertiesMetricEnglishComments
Melting Point 240 °C464 °F
 
Descriptive Properties
Permeation Rate2.0 g-mm/m2-24hr

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AGC Fluon® AH-2000 LM-ETFE, Non-Conductive Type, Fluororesin
Overview of materials for Polyphenylene Sulfide (PPS), Conductive
GEHR Plastics PVDF Polyvinylidene Fluoride
Daikin NEOFLON® RP-5000AS Tubing Grade EFEP
AGC Fluon® LM-740AP LM-ETFE Fluororesin

PAGC19 / 22978

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.