MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

MRC Polymers MAXNITE™ 500 GF15 PET, 15% Glass Fiber Filled  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), 20% Glass Reinforced

Material Notes:

Information provided by MRC Polymers Inc.

Key Words: PET
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.43 g/cc1.43 g/ccASTM D792
Filler Content 15 %15 %+/- 2%; ASTM D2584
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 82.7 MPa12000 psiASTM D638
Elongation at Break 2.0 %2.0 %ASTM D638
Flexural Strength 131 MPa19000 psiASTM D790
Flexural Modulus 5.86 GPa850 ksiASTM D790
Izod Impact, Notched 0.641 J/cm
@Temperature 22.8 °C
1.20 ft-lb/in
@Temperature 73.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 210 °C410 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 260 - 282 °C500 - 540 °F
Middle Barrel Temperature 260 - 288 °C500 - 550 °F
Front Barrel Temperature 266 - 288 °C510 - 550 °F
Nozzle Temperature 271 - 299 °C520 - 570 °Freverse tapered recommended
Melt Temperature 271 - 293 °C520 - 560 °F
Mold Temperature 82.2 - 104 °C180 - 220 °Fthick wall - thin wall
Drying Temperature 116 - 135 °C240 - 275 °F
Dry Time 4 - 6 hour4 - 6 hour
Moisture Content <= 0.020 %<= 0.020 %
Dew Point <= -17.8 °C<= 0.000 °F
Drying Air Flow Rate 22.7 - 28.3 l/min0.800 - 1.00 ft³/min (CFM)per lb/hour resin processed
Injection Pressure 68.9 - 138 MPa10000 - 20000 psi
Back Pressure 0.345 - 1.21 MPa50.0 - 175 psikeep minimum
Cushion 0.635 cm0.250 in
Screw Speed 20 - 50 rpm20 - 50 rpm
 
Descriptive Properties
DryerDehumidified hopper
Fill RateModerate-Fast
Hold Pressure40-60% of injection pressure
Packing Pressure50-75% of injection pressure

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Celcon® LU-02 POM, UV Resistant
Bisalloy Steels BisPlate 80PV Thickness 6-<16 mm
Ineos Nova Zyntar® 779 High Performance Flame Retardant Polystyrene
UCAR Carbon UCAR® PGW Pressure Molded Graphite
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced

PMRC009 / 89438

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.