ZOLTEK’s PX35 Milled Fibers are specifically processed PAN (polyacrylonitrile) based fibers for lower cost applications. All ZOLTEK milled products are free of any sizings. ZOLTEK’s in-house milling system ensures product quality and traceability from raw material through finished product. APPLICATIONS: • RFI/EMI shielding of electronic devices • Buoyancy • Static dissipation • Resin-rich surface reinforcement in composites • Low-cost friction compounds. Information provided by Zoltek Corporation. |