MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Abatron LiquidWood® Deep Penetrating Wood Consolidant
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: LiquidWood® is a deep penetrating wood consolidant that regenerates and waterproofs rotted, dried-out, or spongy wood. It restores structural strength and durability to wood fibers. With LiquidWood®, a piece of deteriorated wood that could crumble under finger pressure can be impregnated and restored to a rigid, durable, water and weather resistant wood superior to the original. The hardened mass can be sawed, planed, routed, carved, drilled, nailed, sanded, glued, and painted. LiquidWood® is also a primer for WoodEpox®. LiquidWood® is ideal for regenerating and waterproofing rotted, dried-out, or spongy window sills, thresholds, window and door frames, columns, stair steps, balustrades, floors, capitals, moldings, doors, shutters, indoor and outdoor furniture, archaeological and art restoration, boats, and millwork of all kinds. LiquidWood® has exceptional adhesion, structural strength, versatility, permanence, dimensional stability, and water resistance. LiquidWood® A and B are easy-to-use, are 100% reactive compounds, and contain no VOC's or noxious odors. Contents ? LiquidWood® consists of 2 clear, epoxy liquids: resin (A) and hardener (B). When A and B are mixed together in equal volumes, by simple stirring, a blend is formed with unique properties to impregnate and restore wood and other porous masses. Application ? Pour on brush on the wood where it penetrates the fibers and hardens into a water-resistant, distortion-free, high-strength mass in hours or minutes. 100% solids. 1/1 ratio. 30 minute pot life.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 100 %100 %
Volatile Organic Compounds (VOC) Content 0.00 g/l0.00 g/l
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4242
Tensile Strength at Break 10.1 MPa1460 psi
Elongation at Break 84 %84 %
Flexural Strength 6.21 MPa900 psi
Compressive Strength 35.9 MPa5210 psi
 
Processing PropertiesMetricEnglishComments
Pot Life 30 min30 min

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Abatron WoodEpox® Wood Replacement Compound
Diamond, Natural
Diamond, Synthetic
Reade Advanced Materials Wood's Metal Alloy (Sn + Pb + Bi + Cd)
A. Schulman POLYBATCH™ Norwegian Wood 60242U/3 Concentrate Based In LLDPE

PABC883 / 107867

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.