MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis Fibremod™ GB402HP 40% Long Glass Fiber Reinforced Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 40% Glass Fiber Filler

Material Notes: GB402HP is a 40% long glass fiber reinforced polypropylene grade, produced using Borealis ` propriety and exclusive, patented Nepol technology intended for injection molding and extrusion. The long glass fibers, chemically coupled to the polypropylene matrix, are providing Nepol GB303HP with outstanding mechanical properties such as high strength, high stiffness and excellent impact resistance.

GB402HP has been designed for front end carriers, structural parts, dashboard carriers, door module carriers, and lead bearing automotive parts.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³ISO 1183
Linear Mold Shrinkage 0.0040 cm/cm0.0040 in/inBorealis Method
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break 2.0 %2.0 %ISO 527-2
Tensile Modulus 9.00 GPa1310 ksiAt 1 mm/min; ISO 527-2
Flexural Modulus 8.40 GPa1220 ksiAt 2 mm/min; ISO 178
Charpy Impact Unnotched 5.70 J/cm²27.1 ft-lb/in²ISO 179/1eU
 5.50 J/cm²
@Temperature -20.0 °C
26.2 ft-lb/in²
@Temperature -4.00 °F
ISO 179/1eU
Charpy Impact, Notched 2.80 J/cm²13.3 ft-lb/in²ISO 179/1eA
 3.20 J/cm²
@Temperature -20.0 °C
15.2 ft-lb/in²
@Temperature -4.00 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 162 °C324 °FISO 75-2
Vicat Softening Point 145 °C293 °FB (50N); ISO 306
 
Processing PropertiesMetricEnglishComments
Front Barrel Temperature 220 - 240 °C428 - 464 °F
Melt Temperature 240 - 270 °C464 - 518 °F
Mold Temperature 60.0 - 100 °C140 - 212 °F
Screw Speed 30 - 150 rpm30 - 150 rpm
 
Descriptive Properties
Fogging, mg1.7At 100°C/ 16 hours

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis Fibremod™ GB303HP 30% Long Glass Fiber Reinforced Polypropylene
PlastiComp Complet® LGF40 - PP Homopolymer Polypropylene, 40% Long Glass Fiber Reinforced
Borealis Nepol™ GB601HP Polypropylene, 30% Long Glass Fiber Reinforced w/HK060AE
A. Schulman Diamond NPP25-0504LGF40 40% Long Glass Fiber Filled Copolymer Polypropylene
Overview of materials for Polypropylene with 50% Glass Fiber Filler

PBOREA183 / 27490

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.