MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Rogers Arlon R36319R028 Silicone Rubber/Fiberglass Laminate
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber; Silicone, Molded, Glass Fiber Filled

Material Notes: Interleave: 3 mil PE; Layer 2: uncured silicone rubber; Layer 1: Cured silicone rubber; Substrate: 162 fiberglass

Information provided by Arlon Silicone Technologies; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.38 g/cc1.38 g/ccArlon SQA-TMS-024
Thickness 127 microns5.00 millayer 1; Arlon SQA-TMS-003
 152 microns6.00 millayer 2; Arlon SQA-TMS-003
 432 microns17.0 milsubstrate; Arlon SQA-TMS-003
 711 microns28.0 miloverall; Arlon SQA-TMS-003
Outgassing - Total Mass Loss 0.34 %0.34 %post cured; ASTM E 595
 1.07 %1.07 %no post cure; ASTM E 595
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4848silicone property; ASTM D2240
Tensile Strength, Ultimate 5.86 MPa850 psiASTM D412
Elongation at Break 450 %450 %silicone property; ASTM D412
Adhesive Bond Strength 0.103 MPa15.0 psiArlon SQA-TMS-047
Tear Strength 12.3 kN/m70.0 pliDie B; silicone property; ASTM D624
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 14.4 kV/mm365 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 232 °C450 °F
Minimum Service Temperature, Air -56.7 °C-70.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 120 min
@Temperature 218 °C
2.00 hour
@Temperature 425 °F
 15.0 min
@Pressure 0.345 MPa,
Temperature 121 °C
0.250 hour
@Pressure 50.0 psi,
Temperature 250 °F
Shelf Life 6.00 Month
@Temperature 23.9 °C
6.00 Month
@Temperature 75.0 °F
 
Descriptive Properties
ColorRed
Outgassing - CVCM (%) ASTM E5950.1post cured
 0.28no post cure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexWeb® HRH-327 - 3/16 - 5.0 Fiberglass Reinforced Polyimide Honeycomb
Overview of materials for Thermoset Polyurethane, Elastomer, Glass Filled
Rogers Arlon 56976XA026 Silicone Rubber/Fiberglass Laminate
Rogers Arlon A3020-T004-12 Silicone Rubber/Fiberglass Laminate
Rogers Arlon R37881R015 Silicone Rubber/Fiberglass

PARL056 / 79708

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.