MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Taiwan PU SITB0302 Silicone Tube
Categories: Polymer; Thermoplastic; Silicone, Thermoplastic

Material Notes: Key features:
  • Excellent electrical properties
  • Very wide service temperature range
  • High flexibility
  • Anti-aging
  • Peroxide cured silicone tube
Application: Silicone tube is flexible, durable and good in temperature resistance to make it as ideal tube for a wide variety of industries. Silicone tube is most commonly used as electrical sleeving, medical equipment, protective cover of lighting, computer applications. Silicone tube is perfect for food processing, pharmaceutical industries and dairy industry.

Information provided by Taiwan PU Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Linear Mold Shrinkage 0.026 cm/cm0.026 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5858
Tensile Strength 6.89 MPa1000 psi
Elongation at Break 260 %260 %
100% Modulus 0.214 MPa31.0 psi
Resilience 5555Rebound
Tear Strength 12.0 kN/m68.5 pli
Compression Set 38 %
@Temperature 80.6 °C,
Time 79200 sec
38 %
@Temperature 177 °F,
Time 22.0 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTAIWPU290 / 306020

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.