MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

DuPont Elvaloy® PT Ethylene/N-Butyl Acrylate/Glycidyl Methacrylate Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Ethylene Butyl Acrylate

Material Notes: Specialized copolymers deliver flexibility, toughness and weatherability to adhesives, plastics, highways and roofing.

Availability: Globally

Information provided by DuPont.

This product line/trade name was acquired by Dow, but this specific grade was discontinued prior to the acquisition.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³ASTM D792 - ISO 1183
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 190 °C
12 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238 - ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7373ASTM D2240 - ISO 868
Tensile Strength at Break 5.20 MPa754 psiASTM D638 - ISO 527-2
Elongation at Break 950 %950 %ASTM D638 - ISO 527-2
 
Thermal PropertiesMetricEnglishComments
Melting Point 72.0 °C162 °FASTM D3418 - ISO 3146
Glass Transition Temp, Tg -55.0 °C-67.0 °FASTM D3418

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Elvaloy® PTW Ethylene/N-Butyl Acrylate/Glycidyl Methacrylate Copolymer
DuPont Elvaloy® AS Ethylene/N-Butyl Acrylate/Glycidyl Methacrylate Copolymer
Overview of materials for Ethylene Butyl Acrylate
Arkema LOTRYL® 29 MA 03 Copolymer Ethylene - Methyl Acrylate
Dow Elvaloy® HP441 Ethylene/N-Butyl Acrylate/Carbon Monoxide Copolymer

PDUPM047 / 33714

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.