MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Syensqo (Solvay Specialty Polymers) Diofan® B 204 PVDC
Categories: Polymer; Thermoplastic; Polyvinyl Dichloride (PVDC); Polyvinyl Dichloride (PVDC)

Material Notes: Diofan® B 204 is a PVDC water-based dispersion with outstanding impermeability to gases and moisture. It is particularly recommended for coatings on plastic films.

Applications: Coating ApplicationsDiofan® B 204 is delivered in bulk or in Intermediate Bulk Containers (IBC). Bulk supplied latex should be stored in reservoirs made of suitable stainless steel, HDPE, rigid PVC or glass fiber-reinforced polyester.
- Contact of anionic Diofan® dispersion with metals like iron, zinc, aluminum and copper as well as alloys such as brass and bronze must be avoided.
- Keep the vessels tightly closed to prevent drying through evaporation. Store the product ideally between 5°C and 30°C (41 °F and 86°F) to avoid degradation.

PROCESSING - DRYING
- Diofan® B 204 can be processed with different coating techniques, including reverse gravure roll and air knife coating systems.
- When coated on plastic films, Diofan® B 204 should be formulated with wax and silica in order to improve the blocking and slip properties of the finished coating.
- Diofan® coatings requires adequate drying conditions, since in general higher temperatures will contribute to better barrier properties.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.27 g/cc0.0459 lb/in³
pH 1.51.5
Water Vapor Transmission 11.0 g/m²/day
@Thickness 0.00100 mm,
Temperature 38.0 °C
0.708 g/100 in²/day
@Thickness 0.0000394 in,
Temperature 100 °F
90% RH; ASTM F1249
Viscosity 17 cP
@Temperature 20.0 °C
17 cP
@Temperature 68.0 °F
 
Mechanical PropertiesMetricEnglishComments
Coefficient of Friction, Dynamic 0.350.35vs. Itself; ASTM D1894
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorMilky White
FormsLiquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4173 / 279973

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.