MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP Radel R-7625 Polyphenyl Sulfone (PPSU); Flame Retardant
Categories: Polymer; Thermoplastic; Polyphenylsulfone (PPSU)

Material Notes: Aircraft interior grade material. Complies with AITM 2.0007 & BSS 7238 test methods for Smoke Density, <200 Ds@4min in the flaming mode. Complies with AITM 3.0005 & BSS 7239 for Toxic Gas Emission at 4 minutes. Complies with OSU 55/55 Heat Release (2 Minute Test) per FAR 25.853.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.36 g/cc1.36 g/ccASTM D 792
Water Absorption 0.30 %
@Time 86400 sec
0.30 %
@Time 24.0 hour
ASTM D 570
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm
@Thickness 3.20 mm
0.0060 - 0.0080 in/in
@Thickness 0.126 in
ASTM D 955
Melt Flow 17 g/10 min
@Load 2.16 kg
17 g/10 min
@Load 4.76 lb
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 86.2 MPa12500 psiASTM D 638
Elongation at Break 30 %30 %ASTM D 638
Tensile Modulus 2.83 GPa410 ksiASTM D 638
Flexural Strength 121 MPa17500 psiASTM D 790
Flexural Modulus 2.76 GPa400 ksiASTM D 790
Izod Impact, Notched 0.694 J/cm
@Thickness 3.20 mm
1.30 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched NB
@Thickness 3.20 mm
NB
@Thickness 0.126 in
ASTM D 4812
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 193 °C380 °FASTM D 648
Flame Spread 25.4 mm/min
@Thickness 1.50 mm
1.00 in/min
@Thickness 0.0591 in
Aerospace; FMVSS 302
 
Processing PropertiesMetricEnglishComments
Melt Temperature 343 - 377 °C650 - 710 °F
Mold Temperature 135 - 177 °C275 - 350 °F
Drying Temperature 149 °C
@Time 21600 sec
300 °F
@Time 6.00 hour
Moisture Content 0.040 %0.040 %
Dew Point -31.7 °C-25.0 °F
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Westlake Plastics Radel® R 4400 Polyphenylsulfone For Medical Applications
Westlake Plastics Radel® R Polyphenylsulfone
RTP Company RTP Radel R-7700 Polyphenyl Sulfone (PPSU); Flame Retardant
RTP Company RTP Radel R-7400 Polyphenyl Sulfone (PPSU); Flame Retardant
Syensqo (Solvay Specialty Polymers) Radel® RG-5030 Polyphenylsulfone (PPSU)

PQZRA32273 / 206053

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.