MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chevron Phillips Marlex® K607 High Density Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Extruded

Material Notes: High Density Polyethylene

Customer Benefits: This extrusion grade homopolymer has excellent process stability and outstanding stiffness.

Applications: Recommended resin for thin sheet, cut sheet up to 1.5 inches thick, separator panels.

Processing Recommendations:
Extrusion Melt Temperature: Upper Limit: 232°C, Lower Limit: 193°C

Specification Data: ASTM D4976-95 - PE244

Data provided by Chevron Phillips Chemical Company, LP.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.964 g/cc0.0348 lb/in³ASTM D1505
ESCR 100% Igepal® 15 hour15 hourCondition A, F50 (100% Igepal CO-630), ASTM D1693
Melt Flow 0.65 g/10 min0.65 g/10 minCondition 190/2.16; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 30.0 MPa4350 psi2 in per min; ASTM D638 Type IV
Elongation at Break >= 300 %>= 300 %2 in per min; ASTM D638 Type IV
Flexural Modulus 1.654 GPa239.9 ksiASTM D790
 
Processing PropertiesMetricEnglishComments
Processing Temperature 193 - 232 °C379 - 450 °FExtrusion

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Petrothene® LR734045 High Density Polyethylene (Sheet & Profile Extrusion)
LyondellBasell Petrothene® LR734001 High Density Polyethylene, Sheet & Profile Extrusion Data
LyondellBasell Petrothene® KR92717 High Density Polyethylene
LyondellBasell Alathon® L5005 High Density Polyethylene
Dow UNIVAL™ DMDH-6400 NT 7 High Density Polyethylene Resin (HDPE)

PCHEVM28 / 20318

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.