EDRO #5™ H13 is a chromium-molybdenum-vanadium-alloyed steel characterized by: good resistance to thermal shock and thermal fatigue, good high-temperature strength, good toughness and ductility, good machinability, good polishability, good through-hardening properties, and good size stability during hardening.Information provided by EDRO |