MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Momentive Performance Materials PolarTherm® PTX25 Boron Nitride (BN) Powder
Categories: Ceramic; Nitride; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Spherical BN Agglomeration Powder. Spherical nature may improve thermal conductivity at moderate loading levels when used as a filler in polymers or lubricants, and produce less anisotropic properties. Features of BN include thermal conductor, electrical insulator, low dielectric constant, high temperature stability, lubricious, inert, and non-wetting.

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.300 g/cc0.0108 lb/in³Tap Density
Particle Size >= 10 µm>= 10 µmD10
 25 µm25 µmMean
 <= 45 µm<= 45 µmD90
Specific Surface Area 7.0 m²/g7.0 m²/g
 
Descriptive Properties
Carbon0.03%
MorphologySpherical Agglomerate
Oxygen0.2%
Sol. Borate0.1%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Momentive Performance Materials PolarTherm® PT620 Boron Nitride (BN) Powder
Momentive Performance Materials PolarTherm® PTX60 Boron Nitride (BN) Powder
Momentive Performance Materials PolarTherm® PT670 Boron Nitride (BN) Powder
Alumina, alpha Al2O3, 99.5%
Momentive Performance Materials PolarTherm® PT350 Boron Nitride (BN) Powder

CADV74g / 149815

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.