MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Toyobo Vectra® FIT50 LCP, 30% Mineral Fiber Reinforced
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), Mineral Filled

Material Notes: Product Description: Vectra® FIT 50 is a 30% mineral reinforced liquid crystal polymer for injection molding. It has excellent filling capability and extremely low warpage performance in long and thin wall complicated applications.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Good Heat Resistance; High Flow; Low Warpage

Form: Pellets

Processing Method: Injection Molding

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.55 g/cc0.0560 lb/in³ISO 1183
Maximum Moisture Content 0.0100.010
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 90.3 MPa13100 psiISO 527-2/5
Elongation at Break 2.0 %2.0 %ISO 527-2/5
Tensile Modulus 9.03 GPa1310 ksiISO 527-1
Flexural Strength 120 MPa17400 psiISO 178
Flexural Modulus 10.0 GPa1450 ksiISO 178
Flexural Strain at Break 2.4 %2.4 %ISO 178
Charpy Impact Unnotched 2.10 J/cm²10.0 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.273 J/cm²1.30 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  4.21
@Frequency 2.00e+9 Hz
4.21
@Frequency 2.00e+9 Hz
IEC 60250
 4.27
@Frequency 1e+9 Hz
4.27
@Frequency 1e+9 Hz
IEC 60250
Comparative Tracking Index 150 V150 V100 drops; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 11.0 µm/m-°C6.10 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 46.8 µm/m-°C26.0 µin/in-°FISO 11359-2
Specific Heat Capacity 0.000870 J/g-°C0.000208 BTU/lb-°FASTM E1461
Melting Point 128 °C262 °FISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 275 °C527 °FUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 246 °C475 °FUnannealed; ISO 75-2/A
Flammability, UL94  V-0
@Thickness 0.201 mm
V-0
@Thickness 0.00790 in
 V-0
@Thickness 0.406 mm
V-0
@Thickness 0.0160 in
 V-0
@Thickness 0.787 mm
V-0
@Thickness 0.0310 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 20.0 - 30.0 °C68.0 - 86.0 °FHopper
 330 - 340 °C626 - 644 °FHot Runner
Feed Temperature 60.0 - 80.0 °C140 - 176 °FInjection
Rear Barrel Temperature 315 - 325 °C599 - 617 °F
Middle Barrel Temperature 325 - 335 °C617 - 635 °F
Front Barrel Temperature 330 - 340 °C626 - 644 °F
Nozzle Temperature 330 - 340 °C626 - 644 °F
Zone 4 330 - 345 °C626 - 653 °FInjection
Melt Temperature 330 - 345 °C626 - 653 °F
Mold Temperature 80.0 - 120 °C176 - 248 °F
Drying Temperature 150 - 160 °C302 - 320 °F
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hour
Injection Pressure 50.0 - 150 MPa7250 - 21800 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHCQ6322 / 311015

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.