MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Syensqo (Solvay Specialty Polymers) Ixef® 1524 Polyarylamide (PARA), 50% glass fiber
Categories: Polymer; Thermoplastic; Polyarylamide (PAA); Polyarylamide, Glass Fiber Filled

Material Notes: 50% glass fiber, halogen-free flame retardant

Ixef® 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance.

- Natural: Ixef® 1524/0008
- Black: Ixef® 1524/9008
- Custom Colorable

Markets/Uses: Electronics / Mobile Devices Structural / Battery Covers; Electronics / Mobile Devices Structural / Chassis and Frames; Electronics / Mobile Devices Structural / Housings; Electronics / Mobile Devices Structural / Internal Structure Components

Applications: Cell Phones; Electrical/Electronic Applications; Housings

Features: Bromine Free; Chemical Resistant; Creep Resistant; Flame Retardant; Good Dimensional Stability; Halogen Free; High Flow; High Strength; Low Moisture Absorption; Outstanding Surface Finish; Ultra High Stiffness

Injection notes: Hot Runners: 250°C to 260°C (482°F to 500°F)
Injection Pressure: rapid
Storage
Ixef® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Ixef® resins be dried prior to molding following the recommendations found in this datasheet and/or in the Ixef® processing guide.
Drying
This resin should be dried to a target moisture content of less than 0.10%. When using a desiccant air dryer with dew point of -28°C (-18°F) or lower, these guidelines can be followed: 1-2 hours at 120°C (248°F), 2-4 hours at 100°C (212°F), or 2-8 hours at 80°C (176°F).
Injection Molding
IXEF 1524 compound can be readily injection molded in most screw injection molding machines. A general purpose screw is recommended, with minimum back pressure.
The measured melt temperature should be about 270°C (518°F), and the barrel temperatures should be around 250°C to 260°C (482°F to 500°F) in the rear zone, gradually increasing to 260°C to 275°C (500°F to 527°F) in the front zone. If hot runners are used, they should be set to 250°C to 260°C (482°F to 500°F).
To maximize crystallinity, the temperature of the mold cavity surface must be held between 120°C and 140°C (248°F and 284°F). Molding at lower temperatures will produce articles that may warp, have poor surface appearance, and have a greater tendency to creep. Set injection pressure to give rapid injection. Adjust holding pressure and hold time to maximize part weight. Transfer from injection to hold pressure at the screw position just before the part is completely filled (95%-99%).

Information provided by Solvay Specialty Polymers.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.68 g/cc0.0607 lb/in³ISO 1183
Water Absorption 0.30 %
@Time 86400 sec
0.30 %
@Time 24.0 hour
ISO 62
Moisture Absorption at Equilibrium 1.0 %1.0 %50% RH; ASTM D570
 1.3 %1.3 %65% RH; ASTM D570
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm0.0010 - 0.0030 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 230 MPa33400 psiISO 527-2
Elongation at Break 1.9 %1.9 %ISO 527-2
Tensile Modulus 20.0 GPa2900 ksiISO 527-2
Flexural Strength 330 MPa47900 psiISO 178
Flexural Modulus 18.5 GPa2680 ksiISO 178
Charpy Impact Unnotched 4.80 J/cm²22.8 ft-lb/in²Type 1, Edgewise; ISO 179
Charpy Impact, Notched 0.930 J/cm²4.43 ft-lb/in²Type 1, Edgewise, Notch A; ISO 179
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 4.44
@Frequency 2.40e+9 Hz
4.44
@Frequency 2.40e+9 Hz
Method B; ASTM D2250
Dissipation Factor 0.012
@Frequency 2.40e+9 Hz
0.012
@Frequency 2.40e+9 Hz
Method B; ASTM D2250
High Voltage Arc Resistance to Ignition (HVAR) 0.00 - 10 sec0.00 - 10 secPLC 0; UL 746
Comparative Tracking Index >= 600 V>= 600 VIEC 60112
 >= 600 V>= 600 VPLC 0; UL 746
 >= 600 V
@Thickness 3.00 mm
>= 600 V
@Thickness 0.118 in
UL 746
Hot Wire Ignition, HWI 60 - 119 sec60 - 119 secPLC 1; UL 746
 >= 120 sec>= 120 secPLC 0; UL 746
 95 sec
@Thickness 0.400 mm
95 sec
@Thickness 0.0157 in
UL 746
 >= 120 sec
@Thickness 0.750 mm
>= 120 sec
@Thickness 0.0295 in
UL 746
 >= 120 sec
@Thickness 1.50 mm
>= 120 sec
@Thickness 0.0591 in
UL 746
 >= 120 sec
@Thickness 3.00 mm
>= 120 sec
@Thickness 0.118 in
UL 746
High Amp Arc Ignition, HAI 30 - 59 arcs30 - 59 arcsPLC 2; UL 746
 60 - 119 arcs60 - 119 arcsPLC 1; UL 746
 37.6 arcs
@Thickness 0.400 mm
37.6 arcs
@Thickness 0.0157 in
UL 746
 53.6 arcs
@Thickness 0.750 mm
53.6 arcs
@Thickness 0.0295 in
UL 746
 70.2 arcs
@Thickness 1.50 mm
70.2 arcs
@Thickness 0.0591 in
UL 746
 95.4 arcs
@Thickness 3.00 mm
95.4 arcs
@Thickness 0.118 in
UL 746
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min0.000 - 0.394 in/minPLC 0; UL 746
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 227 °C441 °FUnannealed; ISO 75-2/A
Flammability, UL94 V-0
@Thickness 0.400 mm
V-0
@Thickness 0.0157 in
Oxygen Index 37 %37 %ISO 4589-2
Glow Wire Ignition Temperature  775 °C
@Thickness 0.400 mm
1430 °F
@Thickness 0.0157 in
IEC 60695-2-13
 800 °C
@Thickness 0.750 mm
1470 °F
@Thickness 0.0295 in
IEC 60695-2-13
 825 °C
@Thickness 1.50 mm
1520 °F
@Thickness 0.0591 in
IEC 60695-2-13
 850 °C
@Thickness 3.00 mm
1560 °F
@Thickness 0.118 in
IEC 60695-2-13
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 250 - 260 °C482 - 500 °F
Front Barrel Temperature 260 - 290 °C500 - 554 °F
Melt Temperature 280 °C536 °FInjection
Mold Temperature 120 - 140 °C248 - 284 °F
Drying Temperature 100 °C
@Time 3600 - 10800 sec
212 °F
@Time 1.00 - 3.00 hour
 
Descriptive Properties
AdditiveFlame Retardant
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlack; Colors Available
FormsPellets
ProcessingInjection Molding
RoHS ComplianceYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4277 / 280077

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.